Ko te mahi me te pono o ngā hanganga whakarewa i roto i ngā taiao uaua e whakawhirinaki nui ana ki te kōwhiringa o ngā konganuku whakakī tika. Mō te hono i ngā koranu maitai kore waikura e ātete ana ki te pāmahana teitei me te waikura, ko te kōwhiringa o tētahi mea motuhakeNgā Irahiko Whakarewahe mea nui rawa atu. Ko te whakarōpūtanga AWS A5.4 E310-16 e tohu ana i tētahi momo hiko whakarewa maitai kore waikura kounga teitei i hangaia hei whakarato i ngā whakarewa pono me te pakari mō ngā tono wero maha.
Ko tēnei tokotoko whakarewa hikohiko Alloys, e mōhiotia ana ko A402, he hikohiko maitai kore waikura austenitic parakore chromium26-nickel21 me te paninga titania-calcium. Ko te hanganga matū o te tokotoko he mea nui ki tana mahi, e whakarato ana i te ātete tino pai ki te waikura me te waikura i ngā pāmahana teitei, tae atu ki te 2100.°F (1150°C). Mā te nui o te koranu i roto i te waea matua ka mau tonu te hanganga me ngā āhuatanga o te konganuku whakarewa kua whakatakotoria i raro i te ahotea wera.
He āhuatanga matua o tēneiNgā Irahiko Whakarewako tōna paninga me ngā āhuatanga mahi. Mā te paninga titanium-konupūmā ka māmā te patu i te pewa, ka pumau te mura o te pewa, ā, ka iti te tauhiuhi, ka puta he āhua maeneene, he ātaahua hoki te āhua o ngā titi. He tino pai te mahi a te hikohiko i roto i te whakarewanga tūnga katoa, tae atu ki te poutū me te runga, e whakarato ana i te ngāwari nui i te wā hanga me te mahi whakatika. Ko te para ka hiki ake i a ia anō, ā, he ngāwari ki te tango, ka whakarei ake i te pai o te whakarewanga.
Ko te whakamahinga matua o te hiko E310-16 ko te whakarewa i ngā maitai ātete wera momo 25Cr-20Ni, pērā i te HK40 me te 310S. He whānuitia te whakamahinga i roto i te hanga me te tiaki i ngā wāhanga pāmahana-tiketike, tae atu ki ngā wāhanga oumu, ngā ngongo whakahou, me ētahi atu taputapu pyrolysis. He maha ngā wā ka tīpakohia tēnei tokotoko whakarewa hiko koranu mō te whakarewa rerekē i waenga i ngā momo maitai kore waikura rerekē, mō te whakakikorua rānei i ngā mata e hiahia ana ki te ātete pāmahana-tiketike.
E tautuhia ana e te whakarōpūtanga AWS A5.4 E310-16 he mahi-teiteiNgā Irahiko WhakarewaHe mea nui mō ngā ahumahi e tino hira ana te pumau o te wera me te ātete ki te waikura. Nā tōna mahi āwhata pumau me ōna āhuatanga whakarewa whakarewa pai rawa atu, he mea pono tēnei hei whiriwhiri māu hei whakarite i te roa o te ora me te haumaru o ngā rawa pāmahana teitei. Ko te whakamahinga tika o tēnei taputapu whakarewa motuhake he tūāpapa mō te hanga kounga i roto i ngā rāngai hinu me te whakaputa hiko.