He maha ngā kaiwhakarewa rākau e ako ana me te momo hiko kotahi. He mea whai tikanga tēnei. Mā tēnei ka taea e koe te whakapai ake i ō pūkenga me te kore e manukanuka ki ngā tawhā me ngā tautuhinga rerekē. Koinei anō te pūtake o tētahi raruraru urutā i waenga i ngā kaiwhakarewa rākau e rite ana te whakahaere i ia momo hiko. Kia kore ai koe e taka ki te mate, kua kohikohia e mātou te aratohu tino pai mō ngā momo hiko me pēhea te whakamahi.
E6010
He tokotoko Fast Freeze ngā 6010 me te 6011. Ko te tikanga o Fast Freeze ko tāu e whakaaro ai (ngā mihi ki a koe e te tangata whakapūmau). Ka tere ake te whakamatao o ngā hiko Fast Freeze i ētahi atu momo, ā, ka ārai i te pupuhi o te puna wai, ka kore hoki e wera rawa. Ko te tikanga ka taea e koe te whakatakoto i tētahi poroporo angiangi e uru atu ana ki roto i tō wahi mahi. Mā tēnei ka taea e koe te tahu i te waikura me ngā rauemi paru, nō reira kāore koe e hiahia ki te horoi i tō rauemi i mua i te whakapūmau. Ko tētahi mea hei maumahara ko ngā tokotoko 6010 ka mahi noa i runga i te hiko au tika.
E6011
He mea hanga ngā hikohiko, ehara i te mea i whānau mai. Engari mehemea i hangaia, ko te 6011 te tuahine māhanga o te 6010. He tokotoko Fast Freeze rāua, he mea pai mō ngā pūtake pakiaka me te whakarewa paipa. He iti noa te paru e toe ana i roto i te puna whakarewa iti hei ngāwari ki te horoi. Ahakoa i hangaia te 6011 mō ngā mīhini AC, ka taea hoki te whakahaere i runga i te DC, he painga ake tēnei i ngā hikohiko 6010 (ka taea anake te mahi i te hikohiko pai o te au tika).
E6013
Ko tētahi hapa noa mā ngā kaiwhakarewa rakau ko te whakamahi i ā rātou irahiko 6013 kia rite ki ngā tokotoko 6011, 6010 rānei. Ahakoa he rite tonu ētahi āhuatanga, he rite te para o te 6013 ki te rino, ā, he nui ake te kaha e hiahiatia ana hei pana. Ka pōhēhē ngā kaiwhakarewa ina kī tonu ā rātou pītiti i ngā kōhao noke, kāore e mōhio me whakanui ake ā rātou amp. Ka whakaora koe i te nui o te raruraru mā te tohutoro noa i ō tautuhinga e hiahiatia ana i mua i te tīmatanga o te whakamahi i tētahi momo tokotoko hou. He tino māmā, inā koa me tētahi o ā mātou taupānga whakarewa kore utu tino pai (ka kitea e koe i konei). He mea nui hoki kia horoia tō whakarewa i te mea pai rawa atu i mua i te tīmatanga o te whakarewa. He ngawari ake te urunga o te 6013 me te puna nui ake e kore e tapahi i te waikura pērā i te 6010, te 6011 rānei.
E7018
He tino pai tēnei hikohiko ki ngā kaiwhakarewa hanganga nā tōna pewa maeneene. Nā tōna urunga ngawari me te puna nui ake ka waiho he pītiti nui ake, he kaha ake, he iti ake te mārama. Pērā i te 6013, ko te urunga ngawari te tikanga me whai mata ma koe hei whakarewa. Waihoki, he rerekē ngā tawhā o ngā 7018 i ētahi atu tokotoko, nō reira kia tirohia ō tautuhinga i mua i tō tīmatanga.
Ki te nuinga o ngā tohunga, ko te wāhanga tino uaua mō ēnei irahiko ko te penapena tika i a rātou. Kia whakatuwheratia te pouaka, he mea pai kia penapenahia ngā irahiko toenga ki roto i te oumu rakau. Ko te whakaaro kia kaua e uru te makuku ki roto i te wai mā te whakamahana i a rātou ki te 250 nekehanga.
E7024
Ko te 7024 te matua o ngā irahiko, e whakamanamana ana ki te paninga para taumaha, taumaha. Pērā i te 7018, ka waiho he poroporo maeneene pai me te ngawari o te uru, ā, me whai mata rauemi ma kia mahi ai. E rua ngā raruraru noa e kitea ana e ngā tohunga me ngā tokotoko 7024. Tuatahi, kāore e whakamahia e ngā kaiwhakarewa te kaha pewa e ranea ana hei pana i te para, ā, ka mutu he whakarewa e taea ana, ahakoa he koretake. Anō, mā te 5 hēkona tere i runga i te taupānga aratohu tohutoro ka whakaora i a koe i te maha o ngā raruraru. Ko tētahi atu raruraru ko te wā e ngana ana ngā kaiwhakarewa ki te whakamahi i ngā tokotoko 7024 ki ngā whakarewa o runga. Ka huri te para taumaha hei pōro ahi ua, ko te tikanga kāore koe e hiahia ki te tapahi huruhuru mō tētahi wā.
Ae, ahakoa nō ngā waitohu iti iho i te paerewa te whakamahi i ngā tokotoko tika, kāore he aha. Waimarie, e tautoko ana mātou i ā mātou taonga katoa kia pai ai te whakarewa. Tirohia te rerekētanga ka puta mai i tēnei ki ngā tokotoko e hokona ana i ngā toa nui i konei.
Wā tuku: Hakihea-23-2022