Te Aratohu Tino Pai mō ngā Rakau Whakarewa Kowiri tira: AF2209-16 (AWS E2209-16)

I te wā e whakarewahia ana te maitai kore waikura, he mea nui te whakamahi i te hiko tika kia tutuki ai he whakarewa kaha, he whakarewa pakari hoki.AF2209-16 (AWS E2209-16)he hiko e piki haere ana te rongonui i roto i te umanga whakarewa. He hiko maitai kore waikura takirua kei roto he waro tino iti, he hauota, he paninga konupūmā-tiatana, koia te whiringa tuatahi mō ngā mahi whakarewa.

Ngā Rakau Whakarewa Kowiri tira AWS E2209-16, Ngā Rakau Whakakī Hikohiko Kua Taupokina ki te Kowiri tira E2209 (4) E2209 (5)

Kua hangaia te hiko AF2209-16 mō te whakarewa i te maitai kore waikura takirua, e mōhiotia ana mō tōna ātete pai ki te waikura me te kaha teitei. Mā te tāpiri o te hauota ki te hanganga hiko ka āwhina i te whakapai ake i te ātete o te whakarewa ki te waikura poka me te waikura kapiti, kia pai ai te whakamahi i roto i ngā taiao uaua pēnei i te moana me te ahumahi tukatuka matū.

Ko tētahi o ngā āhuatanga matua o te hiko AF2209-16 ko tōna ihirangi waro tino iti, e āwhina ana ki te whakaiti i te hanganga o ngā waro i roto i te konganuku whakarewa, kia mau tonu ai te ātete ki te waikura o te maitai kore waikura. Hei tāpiri, ko te paninga konupūmā titanium i runga i te hiko e whakarato ana i ngā āhuatanga pewa pumau me te tango ngāwari i te paru, ka hua ake he poroporo whakarewa ma, maeneene hoki.

I te whakamahi i te hiko AF2209-16, he mea nui kia whai i ngā tawhā whakarewa kua tūtohutia mō ngā hua pai rawa atu. Kei roto i tēnei ko te whiriwhiri i te amperage, te ngaohiko me te tere haere e tika ana i runga i te matotoru o te maitai kore waikura hei whakarewa. Me whai whakaaro hoki ki ngā maimoatanga i mua me muri i te whakarewatanga, pērā i te whakamahana me te whakakorenga i muri i te whakarewatanga, hei whakarite i te pono o te whakarewatanga me te whakaiti i te tūponotanga o te waikura.

Hei whakarāpopototanga, he kōwhiringa pono ngā hikohiko kowiri tira AF2209-16 (AWS E2209-16) mō te whakarewa i ngā kowiri tira takirua, he ātete pai ki te waikura, he kaha teitei, he ngāwari hoki te whakamahi. Mā te mārama ki tōna hanganga ahurei me te whai i ngā tikanga whakarewa kua tūtohutia, ka taea e ngā kaiwhakarewa te whakatutuki i ngā whakarewa kounga teitei e tutuki ai ngā whakaritenga pakari o ngā momo tono ahumahi. Ahakoa e whakamahia ana hei hanga oko pēhanga, paipa, wāhanga hanganga rānei, he taputapu tino nui te hikohiko AF2209-16 hei whakatutuki i te mahi whakarewa pai rawa atu i roto i ngā tono kowiri tira.


Wā tuku: Pipiri-05-2024