I te wā e whakarewa ana, ko te whāinga he hanga i tētahi hononga kaha, kore he hononga i waenganui i ngā wahi whakarewa e rua. He tukanga maha ngā mahi a te whakarewa MIG e taea ai te whakamahi hei whakarewa i ngā momo konganuku rerekē. He tukanga pai te whakarewa MIG mō te hono i ngā rauemi. Heoi, ki te whakamahia ngā tautuhinga hē, ka taea te whakauru i te porosity ki roto i te whakarewa. Ka raru pea tēnei i te kaha me te pono o te whakarewa.
I roto i tēnei tuhinga, ka tirohia ētahi o ngā take o te porosity i roto i te whakarewa MIG me pēhea te ārai i tēnā.
He aha ngā take o te porosity i roto i te MIG welding?
Ko te porosity he momo hapa whakarewa ka puta i roto i ngā whakarewa. Ka puta mai he rite ki ngā kōhao iti i roto i te whakarewa, ā, ka taea te whakaiti i te hononga i waenga i ngā wahi whakarewa e rua. Ka taea te porosity e ngā āhuatanga maha, tae atu ki:
1) Te Whakakotahitanga Kore-oti
Ka puta tēnei ina kore te pewa whakarewa e rewa katoa te konganuku turanga me te rauemi whakakī. Ka tupu pea tēnei mena kāore te mīhini whakarewa i te whakatakotoria ki te amperage tika, mena rānei kāore te rama whakarewa i te pupuri tata ki te konganuku.
2) Te iti o te kapinga hau
Ka whakamahia e te whakarewa MIG he hau ārai hei tiaki i te whakarewa mai i te hāora me ētahi atu poke. Mēnā he iti rawa te rere o te hau, ka puta pea te porosity. Ka puta pea tēnei mēnā kāore i te tika te whakatakotoranga o te kaiwhakahaere hau, mēnā rānei he turuturu kei roto i te ngongo hau.
3) Te Mauheretanga Hau
Ko tētahi atu take o te porosity ko te mau o te hau. Ka puta tēnei ina mau ngā mirumiru hau i roto i te puna whakarewa. Ka taea tēnei mēnā kāore te rama whakarewa e puritia ki te koki tika, mēnā rānei he nui rawa te hau tiaki.
4) Te paru me ngā poke
Ka taea hoki te whakapūpū i te paru o te konganuku turanga, te rauemi whakakī rānei. Ka taea hoki e te paru, te waikura, te peita, me ētahi atu poke te whakapūpū. Ka taea tēnei te tupu mēnā kāore te konganuku i te ma i mua i te whakarewa, mēnā rānei he waikura, he peita rānei kei runga i te mata. Ka taea e ēnei poke te aukati i te hononga tika o te whakarewa ki te konganuku.
5) Hau Parepare Kāore i te Rawaka
Ko tētahi atu take o te porosity ko te koretake o te hau tiaki. Ka tupu pea tēnei mena he hē te hau e whakamahia ana mō te tukanga whakarewa, mena rānei kāore i te tika te whakatakoto i te rere o te hau.
Me pēhea te ārai i te pūngao i te wā o te mahi whakarewa MIG?
Anei ētahi mea ka taea e koe te mahi hei ārai i te puta o te porosity i te wā o te tukanga whakarewa MIG:
1. Whakamahia ngā tautuhinga tika: Kia tino tika te tautuhinga o tō mīhini whakarewa. Me whakarite te amperage me te ngaohiko kia rite ki ngā tohutohu a te kaihanga.
2. Whakamahia te hau tika: Kia tino whakamahia te hau tika mō tō tukanga whakarewa. Ko te ākoni te mea e whakamahia ana mō te whakarewa MIG.
3. Rere hau: Whakatakotoria te tere rere hau kia rite ki ngā tohutohu a te kaihanga. Mēnā he nui rawa, he iti rawa rānei te hau, ka puta he porosity.
4. Kia tika te koki o te rama: Kia tika te koki o te rama kia kore ai e mau te hau. Me pupuri te rama i te koki 10 ki te 15 nekehanga mai i te mata o te konganuku.
5. Whakamahia he konganuku ma: Kia tino whakamahia he konganuku ma, kāore i poke mō tō whakarewa. Ka taea e te paru, te waikura, te peita rānei i runga i te mata te whakapūpū i te wai.
6. Whakarewahia ki tētahi wāhi hauhautanga: Whakarewahia ki tētahi wāhi hauhautanga hei ārai i te mau o te hau. Ka taea e te hau tiaki te mau i roto i ngā wāhi kua kati.
Ka taea te ārai i te pūngao mā te whai i ēnei tohutohu. Mā te whakamahi i ngā tautuhinga tika me te whakarewa i roto i tētahi wāhi e pai ana te hau, ka taea e koe te karo i tēnei raruraru.
Ngā Rongoā Noa mō te Whakatika i ngā Wera Porosity
Anei ētahi rongoā noa mō te whakatika i ngā whakarewa kua pāngia e te porosity:
1. Te whakarewa anō: Ko tētahi rongoā noa ko te whakarewa anō i te wāhi e pāngia ana. Ka taea tēnei mā te whakarewa i te wāhi e pāngia ana me te amperage teitei ake.
2. Ngā mono pūwero: Ko tētahi atu rongoā noa ko te whakamahi i ngā mono pūwero. He kōpae whakarewa iti ēnei ka whakatakotoria ki runga i ngā kōhao o te whakarewa. Ka taea te hoko i ngā mono pūwero i te nuinga o ngā toa taputapu whakarewa.
3. Te Huri: Ko tētahi atu huarahi ko te huri i te wāhi kua pāngia, ka whakapiri anō. Ka taea tēnei te mahi mā te whakamahi i te huri ā-ringa, i te huri koki rānei.
4. Waea whakarewa: Ko tētahi atu rongoā ko te whakamahi i te waea whakarewa. He waea angiangi tēnei e whakamahia ana hei whakakī i ngā kōhao o te whakarewa. Ka taea te hoko waea whakarewa i te nuinga o ngā toa taputapu whakarewa.
Ka taea te whakatika i te pūngao mā te whakamahi i tētahi o ēnei rongoā noa. Mā te whakarewa anō i te wāhi, mā te whakamahi rānei i ngā mono pūngao, ka taea e koe te whakatika i te raruraru.