Whakaahuatanga Poto:

Ko ngā Rakau Whakarewa Pakari Ārai Konumohe Konumohe A5.13 ECoCr-C e whakamahia ana mō te whakarewa i ngā pane takirere, ngā mowhiti hiri o te papu pēhanga teitei me ngā wāhanga o ngā mīhini kuru.


Taipitopito Hua

Ngā Tohu Hua

ECoCr-A (Cobalt 6) Ko te Hiko Whakarewa Pakari me te Ātete-Kakahu

Momo Koranu: A5.13, PAPA TŌTAKA Ngā Irahiko me ngā Rakau Whakarewa, A5.13
Ko te ECoCr-A Cobalt Alloy 6 te mea e whakamahia whānuitia ana o ngā koranu ātete-kakahu e ahu mai ana i te cobalt, ā, he pai te mahi whānui. E kiia ana ko te paerewa ahumahi mō ngā tono ātete-kakahu whānui, he tino ātete ki ngā momo pirau miihini me te matū i runga i te whānuitanga o te pāmahana, ā, e mau tonu ana te taumata pakeke tae atu ki te 500⁰C (930⁰F). He pai hoki te ātete ki te pānga me te pirau cavitation. He tino pai te Cobalt Alloy 6 mō ngā momo tukanga whakapakeke, ā, ka taea te huri ki ngā taputapu carbide.

Ngā Whakamahinga Noa: ngā mata kutikuti; ngā takirere rere wai; ngā tīwiri whakaputa; ngā pū whakakorikori; te pāmahana teitei; te mata whāriki takirere

Akomanga AWS: ECoCr-A Tiwhikete: AWS A5.13/A5.13M:2010
Koranu: ECoCr-A ASME SFA A5.13

 

Tūnga Whakarewa:
F, V, OH, H
Ināianei:
*NS

 

Kaha Kume, kpsi: *NS
Te Kaha Hua, kpsi: *NS
% Toronga: *NS

*Kāore i te Whakapūtātia te NS

Te Matū Waea Noa e ai ki te AWS A5.13 (ko ngā uara takitahi te mōrahi)

C Mn Si Cr Ni Mo Fe W Co Ētahi atu
0.7-1.4 2.0 2.0 25-32 3.0 1.0 5.0 3.0-6.0 Rem 1.0