ERNiFeCr-1 Nickel Alloy Welding Wire, Nickel Tig Wire Filler Metal

Whakaahuatanga Poto:

Ko te Alloy 825 (ERNiFeCr-1) he waea nickel-rino-chromium e pai ana tenei mo nga momo tono uaua.


Taipitopito Hua

Tohu Hua

Kohanga NikaWaea WeheWaea TigERNiFeCr-1

Paerewa
EN ISO 18274 – Ni 8065 – NiFe30Cr21Mo3
AWS A5.14 – ER NiFeCr-1

 

Nga waahanga me nga tono

Ko te Alloy 825 he anickel-Waea rino-chromium e pai ana tenei mo nga momo tono uaua.

Ko tenei waea e whakarato ana i nga taumata teitei o te aukati i te waikura ki nga taiao whakangao me te whakaiti.

He tino pai mo te whakakikorua i nga waahi e hiahiatia ana te hanganga matū rite.

He pai rawa te weldability me te tino austenitic weld whakarewa me te tino parenga ki te ahotea kapiti waikura i roto i te pāpāho kei roto katote pūhaumāota.

Ka whakamahia i roto i nga umanga tukatuka matū, petrochemical, hanga pepa me te whakaputa hiko etc.

 

Rauemi Turanga Tikanga

G-X7NiCrMoCuNb 25 20, X1NiCrMoCuN25 20 6, X1NiCrMoCuN25 20 5, NiCr21Mo, X1NiCrMoCu 31 27 4, N08926, N08904, ALLOY 82, N08904, ALLOY 82. .4500, 1.4529, 1.4539 (904L), 2.4858, 1.4563, 1.4465 , 1.4577 (310Mo), 1.4133, 1.4500, 1.4503, 1.4505, 1.4506, 1.4531, 1.4536, 1.4585, 1.4586*
* He rarangi whakaahua, ehara i te raarangi tino

 

Hanga matū %

C%

Mn%

Fe%

P%

S%

Si%

 

mōrahi

0.70

22.00

mōrahi

mōrahi

mōrahi

 

0.05

0.90

min

0.020

0.004

0.50

 

 

Cu%

Ni%

Al%

Ti%

Kr%

Mo%

 

2.30

43.00

mōrahi

1.00

22.00

3.00

 

3.00

46.00

0.20

1.20

23.50

3.50

 

 

Nga Taonga Miihini
Te Kaha Toka ≥550 MPa  
Te Kaha Tuku -  
Te whakaroa -  
Te Kaha Paanga -  

He tata tonu nga taonga miihini, ka rereke pea i runga i te wera, te hau maru, nga tawhā fehokotaki me etahi atu mea.

 

Nga hau whakamarumaru

EN ISO 14175 – TIG: I1 (Argon)

 

Nga Turanga Welding

EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG

 

Raraunga Whakapaipai
Diamita Te roa Taumaha  
1.60 mm

2.40 mm

3.20 mm

1000 mm

1000 mm

1000 mm

5 Kg

5 Kg

5 Kg

 

 