Waea Whakarewa Āwhata AWS A5.22 E317LT1-1 mō te Kowiri tira

Whakaahuatanga Poto:

Kua hangaia te Waea Whakarewa Āwhata AWS A5.22 E317LT1-1 mō te ārai hau CO2 100% me te waea whakarewa tūranga-katoa.


Taipitopito Hua

Ngā Tohu Hua

AWS A5.22 E317LT1-1 Rererangi MatuaĀwhataWaea Whakarewa
JIS Z 3323 TS 317L-FC11

Ngā Āhuatanga me te Whakamahinga
Kua hangaia te Waea Whakarewa Āwhata AWS A5.22 E317LT1-1 mō te ārai hau CO2 100% me te waea whakarewa tūranga-katoa.
E whakamahia ana mō te hono i ngā momo maitai kore waikura pērā i te CF-8M me te CF-3M. He tino pai te mahi a te konganuku whakarewa ki te ātete ki te waikura i waenga i ngā porowhita. Ko ngā whakamahinga noa ko te hanga i ngā mea ki tāwāhi, ngā kaipuke matū me ngā ahumahi petro-matū, penupenu me te pepa.

Te Hanganga Matū Noa o te Mea Whakarewa (%)
C 0.027 Mn 1.32 Si0.59 P 0.028 S 0.007 Cr 19.20 Ni 13.14 Mo 3.57
Ngā Āhuatanga Ā-Mīhini Noa o te Mea Whakarewa
Kaha Kume 620MPa Toronga 34%

Ngā tuhipoka mō te whakamahinga: .
1. I mua i te whakarewanga, me horoi te hinu, te waikura, me te makuku i te rauemi turanga, me whai i te kounga tika.
te ārai i te hau i te papa whakarewa.
2. Whakamahia te CO2 parakore 99.8%, neke atu rānei, hei hau tiaki.
3. Puritia te hua kia maroke i te wā e rongoatia ana, e tukuna ana rānei.

I whakatūria a Wenzhou Tianyu Electronic Co., Ltd. i te tau 2000. Kua uru mātou ki te hanga i ngā irahiko whakarewa,ngā tokotoko whakarewa, me ngā taputapu whakarewa mō ngā tau neke atu i te 20.

Ko ā mātou hua matua ko ngā irahiko whakarewa kowiri tira, ngā irahiko whakarewa maitai waro, ngā irahiko whakarewa koranu iti, ngā irahiko whakarewa mata, ngā irahiko whakarewa koranu nikara me te kobalta, ngā waea whakarewa maitai ngawari me te koranu iti, ngā waea whakarewa koranu kore waikura, ngā waea whakaheke hau-ārai, ngā waea whakarewa konumohe, ngā waea whakarewa pewa ruku. ngā waea, ngā waea whakarewa koranu nikara me te kobalta, ngā waea whakarewa parahi, ngā waea whakarewa TIG me te MIG, ngā irahiko tungsten, ngā irahiko keri waro, me ētahi atu taputapu whakarewa me ngā taonga pau.