AWS A5.23: ECM1 Ngā Mea Whakapau mō te Waea Whakarewa Āwhata Ruku

Whakaahuatanga Poto:

AWS A5.23: ECM1, Ko te Waea Awa-Tohu Ruku he waea hikohiko hiato konganuku-matua iti-koranu mō te whakarewa awa-tohu ruku i roto i ngā tono kaha teitei.


Taipitopito Hua

Ngā Tohu Hua

AWS A5.23: ECM1, Waea Pouaka-Tohu Ruku, Rino Koranu-Iti

He waea hiko iti-konumohe te ECM1, he mea hanga ki te konganuku-matua, mō te whakarewa pewa i raro i te wai i roto i ngā tono kaha teitei. Ā, e tutuki ana i te AWS A5.23 matū M1, ā, kua hangaia mō ngā taumata kaha kume neke atu i te 80 ksi.

NGĀ ĀHUATANGA ME NGĀ PAINGA
• Ka taea e te waea whakarewa-matua te tuku i ngā tere whakatakotoranga pai ake ki te whakaritea ki ngā waea totoka i ngā amperahe rite
• He whānui ake te urunga o ngā waea whakarewa ki ngā waea totoka i ngā tawhā whakarewa rite tonu
• He tino pai te pakari o te pānga ki te pāmahana iti i roto i ngā āhuatanga kua oti te whakarewa me ngā āhuatanga kua whakaitihia te ahotea
• He rite tonu ngā whakaritenga hanganga matū o te putunga whakarewa ki ērā o ngā waea totoka EM1
• He pai mō te whakamahi me te whānuitanga o ngā rerenga
• Ka taea te whakanui ake i te tere o te haere hei whakapai ake i te hua
• Āwhina ki te ārai i te tahunga i te wā e whakarewahia ana i ngā iahiko teitei i runga i ngā ara pakiaka me ngā rauemi angiangi.
• Āwhina ki te whakaiti i te mōrearea o te pakaru i roto i ngā tono nui, i ngā taiao ratonga uaua rānei
• He pai hei huarahi whakaputa hua ake i roto i ngā tono maha e whakamahi ana i te waea totoka EM1 (he rite rānei ki te 80 ksi) i tēnei wā
• Ka whakarato i te whānuitanga o te whanaketanga tukanga me te arotau i te mahi o te tono whakarewa

Ngā Ahumahi
Te hanga hanganga me te piriti, ngā taputapu taumaha, te whakaputa hiko, te hanga kaipuke, te takutai moana
Onāianei
Te Irahiko Au Tika Pai (DCEP), Te Irahiko Au Tika Kino (DCEN), Te Irahiko Tauwhitiwhiti (AC)
ROKIROKI
Me rongoa te hua ki roto i te wāhi maroke, kua kati, me roto anō i tōna takai taketake kāore i pakaru