AWS E10015-G Hikohiko Hauwai Tino-Iti J707RH Rakau Whakarewa Rino Koranu Iti

Whakaahuatanga Poto:

Ko te J707RH (AWS E10015-G) he hiko hauwai tino iti te pakari me te paninga hauwai konutai iti.


Taipitopito Hua

Ngā Tohu Hua

Irahiko Whakarewa Rino Koranu Iti

J707RH                               

GB/T E7015-G

AWS E10015-G

 

Whakaahuatanga: He hiko hauwai tino iti te kaha o te J707RH, he paninga hauwai konutai iti. He DCEP (hiko iahiko au tika) te whakamahinga, ā, ka taea te whakarewa i ngā tūranga katoa. He pai te mahi whakarewa. He pai te piko makariri, te ātete ki te pakaru me te ātete ki te pahūtanga o ngā hononga whakarewa. He tino ngāwari, he pakari hoki te konganuku kua whakatakotoria.

Te Whakamahinga: E whakamahia ana mō te whakarewa i ngā hanganga anga, ā, he pai hoki mō te whakarewa i ngā hanganga nui o te maitai kaha-teitei Rp0.2≥590MPa.

 

Te hanganga matū o te konganuku whakarewa (%):

C

Mn

Cr

Si

Ni

Mo

S

P

S + P

≤0.10

1.20 ~ 1.60

0.08 ~ 0.20

0.30 ~ 0.60

1.40 ~ 2.00

0.25 ~ 0.50

≤0.020

≤0.020

≤0.035

 

Ngā āhuatanga hangarau o te konganuku whakarewa:

tūemi whakamātautau

Te kaha o te kume

Mpa

Te kaha o te hua

Mpa

Te whakaroa

%

Uara pānga (J)

-50℃

Kua whakamanahia

≥690

≥590

≥15

≥34

 

Te nui o te hauwai horapa o te konganuku kua whakatakotoria: ≤4.1mL/100g (tikanga chromatography mercury, hau rānei)

Tirotiro hihi-X: tohu I

 

Iahiko e taunakitia ana:

(mm)

Te whānui o te tokotoko

4.0

5.0

(A)

Iahiko Whakarewa

160 ~ 180

180 ~ 220

 

Pānui:

1. Me tunu te hiko mō te 2 hāora i te 400℃ i mua i te mahi whakarewa;

2. He mea nui kia horoia te waikura, te unahi hinu, te wai, me ngā poke i runga i ngā wāhanga whakarewa i mua i te whakarewa;

3. Whakamahia te pewa poto i te wā e whakarewa ana. He tika te ara whakarewa whaiti.

 


  • O mua:
  • Panuku: