AWS E8016-B2 Irahiko Whakarewa Rino Ātete-Wera R306 Ngā Rakau Whakarewa Rākau Rauemi Whakarewa Hauwai Iti

Whakaahuatanga Poto:

Ko te R306 (AWS E8016-B2) he hiko maitai ātete-wera pearlitic me te paninga pāhare pāporo iti-hauwai kei roto ko te 1% Cr – 0.5% Mo.


Taipitopito Hua

Ngā Tohu Hua

Molybdenum me te Chromium Molybdenum Rino Ātete WeraWhakarewaIrahiko

R306                                                     

GB/T E5516-B2

AWS A5.5 E8016-B2

Whakaahuatanga: He hiko maitai ātete-wera pearlitic te R306, he paninga pāhare pākawa iti-hauwai kei roto ko te 1% Cr – 0.5% Mo. Ka taea te whakamahi i te AC me te DC, ā, ka taea te whakarewa i ngā tūranga katoa. Me whakamahana te whakarewa ki te 160 ~ 250°C i mua i te whakarewa.

Taupānga: Whakamahia mō te whakarewa i te maitai ātete-wera Cr 1% – Mo 0.5%, ā, kei raro iho i te 520℃ te pāmahana mahi, pērā i ngā paipa kōhua, ngā oko pēhanga, ngā mīhini whakamahana me ngā taputapu whakamahine hinu, me ētahi atu.

 

Te hanganga matū o te konganuku whakarewa (%):

C

Mn

Si

Cr

Mo

S

P

0.05 ~ 0.12

0.50 ~ 0.90

≤0.60

0.80 ~ 1.50

0.40 ~ 0.65

≤0.030

≤0.030

 

Ngā āhuatanga hangarau o te konganuku whakarewa:

tūemi whakamātautau

Te kaha o te kume

Mpa

Te kaha o te hua

Mpa

Te whakaroa

%

Uara pānga (J)

Te Mahana Noa.

Kua whakamanahia

≥540

≥440

≥17

≥47

 

Iahiko e taunakitia ana:

Te whānui o te tokotoko

(mm)

2.5

3.2

4.0

5.0

Iahiko Whakarewa

(A)

60 ~ 90

90 ~ 130

140 ~ 180

180 ~ 210

 

Pānui:

1. Me tunu te hiko mō te 1 hāora i te pāmahana tata ki te 350℃ i mua i te mahi whakarewa;

2. He mea nui kia horoia te waikura, te unahi hinu, te wai, me ngā poke i runga i ngā wāhanga whakarewa i mua i te whakarewa.

 

 