Waea Rerekē-Matua E2553T1-1/4 AP
WHAKARĀPOPOTONGA
AWS 5.22 Akomanga E2553T1-1 me E2553T1-4 / ASME SFA 5.22 Akomanga E2553T1-1 me E2553T1-4
UNS# W39533 A#8 F#6
WHAKAMĀRAMA
He waea hiko-matua katoa te E2553T1-4, ā, kua hangaia kia rere ki te 75% Ar / 25% CO2.
He mea hanga tēnei waea kia tino pai te tango i te paru, ā, ka rere pai me te whakawhiti porowhita kāore he tauhiuhi.
NGĀ TONO
E whakamahia ana te waea E2553T1-4 AP he pūtake-rerenga hei hono i ngā koranu maitai kore waikura takirua me te 25% Chromium pea.
Ka whakakotahihia e ēnei koranu kowiri tira takirua te kaha kume me te kaha whakaputa me te ātete pai ake ki te pakaru, te waikura, me te pakaru waikura ahotea. Ko ēnei whakaritenga e kitea whānuitia ana i roto i ngā ahumahi moana, matū, me te hinu.
Mena e hiahiatia ana te whakamahana i muri i te whakarewanga, ka nui ake te pāmahana whakamahana e hiahiatia ana mō tēnei konganuku whakarewa i tērā e hiahiatia ana e te konganuku turanga takirua.
TE TIKANGA
Kāore e hiahiatia he whakamahana. Ko te pāmahana mōrahi i waenganui i te huarahi he 300°F.
Tērā pea e hiahiatia te whakawerawera kia ōrite ai te pakeke o ngā whakarewanga maha-haerenga.
Me whakawhāiti te wera e whakaurua ana ki te 5-40 KJ/IN.
MATUA NOA
| C | Cr | Ni | Mo | Mn | Si | P | S | N | Cu |
| 0.02 | 25.3 | 9.8 | 3.37 | 0.80 | 0.70 | 0.03 | 0.015 | 0.14 | 1.87 |
NGĀ ĀHUATANGA MĪHINI NOA
| PAKARIKI | 25 RC i te mea kua whakarewaina 35 RC i whakapakeketia |
| KAHA TŪTURU | 110,000 PSI Iti rawa |
| TE WHAKAROA | 15% iti rawa |
NGĀ TAWHITO WHAKAPĀ
| RAHI | NGAOHIO | ĀPERA | HAUREHU |
| .045” | 25-30 | 130-220 | 75% Ar / 25% CO2, 100% CO2 rānei |
I whakatūria a Wenzhou Tianyu Electronic Co., Ltd. i te tau 2000. Kua uru mātou ki te hanga i ngā irahiko whakarewa,ngā tokotoko whakarewa, me ngā taputapu whakarewa mō ngā tau neke atu i te 20.
Ko ā mātou hua matua ko ngā irahiko whakarewa kowiri tira, ngā irahiko whakarewa maitai waro, ngā irahiko whakarewa koranu iti, ngā irahiko whakarewa mata, ngā irahiko whakarewa koranu nikara me te kobalta, ngā waea whakarewa maitai ngawari me te koranu iti, ngā waea whakarewa koranu kore waikura, ngā waea whakaheke hau-ārai, ngā waea whakarewa konumohe, ngā waea whakarewa pewa ruku. ngā waea, ngā waea whakarewa koranu nikara me te kobalta, ngā waea whakarewa parahi, ngā waea whakarewa TIG me te MIG, ngā irahiko tungsten, ngā irahiko keri waro, me ētahi atu taputapu whakarewa me ngā taonga pau.