Waea Whakarewa AWS E70T-1 CO2 Ārai-Hauhanga Rererangi

Whakaahuatanga Poto:

Waea Whakarewa AWS E70T-1 CO2 Ārai-Hauhanga. Whakamahia mō te whakarewa i ngā hanganga i hangaia ki te maitai waro me te maitai hanganga iti-koranu he kaha kume teitei ake i te 490MPa, he ōrite rānei.


Taipitopito Hua

Ngā Tohu Hua

AWS E70T-1 Parenga-hau CO2Rererangi Matua Waea Whakarewa

Whakamahia mō te whakarewa i ngā hanganga i hangaia ki te maitai waro me te maitai hanganga iti-koranu me te kaha kume teitei ake i te 490MPa, ōrite rānei. E whakamahia whānuitia ana mō te whakarewa i ētahi hanganga matua pēnei i te hanga kaipuke, te hanga miihini, ngā oko pehanga, ngā kohua, ngā mīhini hinu, ngā mīhini matū, ngā mīhini hiki, me ētahi atu.

Rahi 0.8mm 1.0mm 1.2mm 1.6mm 2.0mm 2.4mm 3.0mm 3.2mm 4.0mm
Ngā tono Whakamahia mō te whakarewa i ngā hanganga i hangaia ki te maitai waro me te maitai hanganga iti-koranu me te kaha kume teitei ake i te 490MPa, ōrite rānei. E whakamahia whānuitia ana mō te whakarewa i ētahi hanganga matua pēnei i te hanga kaipuke, te hanga miihini, ngā oko pehanga, ngā kohua, ngā mīhini hinu, ngā mīhini matū, ngā mīhini hiki, me ētahi atu.

 

Te hanganga matū o te konganuku kua whakatakotoria (%)
C
≤0.18
Si
≤0.90
Mn
≤1.75
S
≤0.03
P
≤0.03

 

I whakatūria a Wenzhou Tianyu Electronic Co., Ltd. i te tau 2000. Kua uru mātou ki te hanga i ngā irahiko whakarewa,ngā tokotoko whakarewa, me ngā taputapu whakarewa mō ngā tau neke atu i te 20.

Ko ā mātou hua matua ko ngā irahiko whakarewa kowiri tira, ngā irahiko whakarewa maitai waro, ngā irahiko whakarewa koranu iti, ngā irahiko whakarewa mata, ngā irahiko whakarewa koranu nikara me te kobalta, ngā waea whakarewa maitai ngawari me te koranu iti, ngā waea whakarewa koranu kore waikura, ngā waea whakaheke hau-ārai, ngā waea whakarewa konumohe, ngā waea whakarewa pewa ruku. ngā waea, ngā waea whakarewa koranu nikara me te kobalta, ngā waea whakarewa parahi, ngā waea whakarewa TIG me te MIG, ngā irahiko tungsten, ngā irahiko keri waro, me ētahi atu taputapu whakarewa me ngā taonga pau.