E71T-11 Waro Rino Rererangi Āwhata Whakarewa Āwhata Waea Whakarewa Rererangi

Whakaahuatanga Poto:

He waea ārai-ā-ia anō te E71T-11, he anga rere tōna, e whakamahia ana mō te whakarewa i ngā maitai waro.


Taipitopito Hua

Ngā Tohu Hua

E71T-11 A5.20, RINO WARORererangi MatuaNgā Irahiko Whakarewa Āwhata

He waea ārai-ā-ia-anō te E71T-11, he mea whakamahi mō te whakarewa i ngā maitai waro. Kāore e hiahiatia he hau ārai, ā, ka taea te whakamahi i roto i ngā mahi whakarewa maha-haerenga iti.

Ngā Whakamahinga Noa: ngā whakarewanga o te pū, te kopa me te muka i runga i te maitai 16 ine ki te ½”; te whakarewanga huihuinga me te tiaki; ngā wāhanga mīhini, ngā tāke, te hanganga o mua

Akomanga AWS: E71T-11 Tiwhikete: AWS A5.20/A5.20M:2005
Koranu: E71T-11 AWS/ASME SFA A5.20

 

Tūnga Whakarewa:
H, F, V-ake, O
Ināianei:
DCEN

 

Kaha Kume, kpsi: 70-95
Te Kaha Hua, kpsi: 58 meneti
% Toronga: 20 meneti

Te Matū Waea Noa e ai ki te AWS A5.9 (ko ngā uara takitahi te mōrahi)

C Mn Si S P Al  
0.30 1.75 0.60 0.03 0.03 1.80  
  Ngā Tawhā Waea Noa
Diameter Tūnga Tukanga Ngā Whakakaha Ngā Waohiko Tere Whāngai Waea
in (mm)  
.030″ 0.8 Tūnga Katoa FCAW 25 14 55
    Tūnga Katoa FCAW 125 16 225
.035″ 0.9 Tūnga Katoa FCAW 55 17 75
    Tūnga Katoa FCAW 80 19 110
    Tūnga Katoa FCAW 120 20 160
.045″ 1.2 Tūnga Katoa FCAW 115 15 105
    Tūnga Katoa FCAW 130 16 125
    Tūnga Katoa FCAW 160 17 170
    Tūnga Katoa FCAW 200 18 195
1/6″ 1.6 Tūnga Katoa FCAW 160 17 70
    Tūnga Katoa FCAW 190 18 100
    Papatahi & Whakapae FCAW 210 19 110
    Papatahi & Whakapae FCAW 260 20 145
0.068 1.7 Tūnga Katoa FCAW 145 18 50
    Tūnga Katoa FCAW 155 18 60
    Tūnga Katoa FCAW 185 18 70
    Tūnga Katoa FCAW 240 18 100
    Papatahi & Whakapae FCAW 255 21 111
    Papatahi & Whakapae FCAW 315 22 160
5/64 2.0 Tūnga Katoa FCAW 185 16 55
    Tūnga Katoa FCAW 190 18 60
    Tūnga Katoa FCAW 220 19 70
    Papatahi & Whakapae FCAW 26 21 90
    Papatahi & Whakapae FCAW 315 22 124

 

 

I whakatūria a Wenzhou Tianyu Electronic Co., Ltd. i te tau 2000. Kua uru mātou ki te hanga i ngā irahiko whakarewa,ngā tokotoko whakarewa, me ngā taputapu whakarewa mō ngā tau neke atu i te 20.

Ko ā mātou hua matua ko ngā irahiko whakarewa kowiri tira, ngā irahiko whakarewa maitai waro, ngā irahiko whakarewa koranu iti, ngā irahiko whakarewa mata, ngā irahiko whakarewa koranu nikara me te kobalta, ngā waea whakarewa maitai ngawari me te koranu iti, ngā waea whakarewa koranu kore waikura, ngā waea whakaheke hau-ārai, ngā waea whakarewa konumohe, ngā waea whakarewa pewa ruku. ngā waea, ngā waea whakarewa koranu nikara me te kobalta, ngā waea whakarewa parahi, ngā waea whakarewa TIG me te MIG, ngā irahiko tungsten, ngā irahiko keri waro, me ētahi atu taputapu whakarewa me ngā taonga pau.