I runga i te piripono ki te ariā o te "kounga, ngā ratonga, te mahi me te tipu", kua riro mai i a mātou ngā whakawhirinaki me ngā whakamoemiti mai i ngā kaihoko o te whare me te ao whānui mō te hokohoko wera mō te Rhk 2.5mm 3.2mm 4.0mm 5.0mm Aws E7018 Waro Rino Āwhata Wera Hiko, ko tā mātou tumanako ka taea e mātou te whai hononga pai ki ngā kaipakihi o te ao katoa.
I runga i te whakapono ki te ariā o "te kounga, ngā ratonga, te mahi me te tipu", kua riro mai i a mātou ngā whakawhirinaki me ngā whakamoemiti mai i ngā kaihoko o te kāinga me te ao whānui mōHaina E7018 Hiko Whakarewa me te Hiko Whakarewa E7018, E mihi ana mātou ki te whai wāhi ki te mahi pakihi ki a koe, ā, e tumanako ana mātou ki te tāpiri atu i ētahi atu taipitopito mō ā mātou hua me ā mātou otinga. Ka taea te whakamana i te kounga pai, te utu whakataetae, te tuku i te wā tika me te ratonga pono. Mō ētahi atu pātai, kaua e mangere ki te whakapiri mai ki a mātou.
NGĀ TONO:
Te whakarewanga o ngā maitai 9% Cr-1% Mo me ngā maitai 9% Cr – 2% Mo e whakamahia ana mō te hiko me te oko pēhanga teitei.
NGĀ WHAKAMĀRAMATANGA:
He hiko iti-hauwai te PA-8016-B8, ā, ko tōna konganuku whakarewa he 9%Cr-1%Mo. He mea hanga mō te maitai pāmahana teitei me ngā maitai mō ngā ratonga hauwai wera, inā koa i roto i te umanga hinu-matū. Ka taea te whakaae i te hiko mō tōna kaha kume teitei, tōna pakari pai me tōna ātete wera nui.
NGĀ TUHIPOKA MŌ TE WHAKAMAHINGA:
1. Whakamarokehia ngā irahiko ki te 350-400°C mō te haora kotahi i mua i te whakamahinga, ā, rongoatia ngā irahiko ki te 100-150°C i muri i te whakamaroketanga, kia tūpato hoki kia kore ai e makuku.
2. Whakamahia te tikanga hikoi whakamuri, te patu rānei i te pewa ki runga i tētahi pereti rino iti kua whakaritea mō tēnei kaupapa hei ārai i ngā pūha i te tīmatanga o te pewa.
3. Kia poto te pewa.
4. Whakamahanahia ki te 100-150°C. Ka rerekē te pāmahana e whakamahia ana i runga i te matotoru o te pereti me te momo maitai e whakarewaina ana.
5. Kia tūpato kei hipa atu i te wera e tika ana, nā te mea ka heke te kaha o te whakarewa whakarewa ki te nui rawa o te wera.
IV. TE HANGA MATUA NOA O TE MEA WHAKAPĀ (%):
| C | Si | Mn | Cr | Mo |
| 0.06 | 0.42 | 0.68 | 9.38 | 1.05 |
V. NGĀ ĀHUATANGA MĪHINI NOA O TE MEA WHAKAPĀ:
| Kaha Kume N/mm2(Ksi) | Pūwāhi Hua N/mm2 (Ksi) | % Toronga | PWHT |
| 705 (102) | 560 (81) | 24 | 740°C x 1 hāora |
VI. NGĀ TŪRANGA WHAKAPĀ: NGĀ TŪRANGA KATOA
VII. TE RAHI ME TE AWHE O TE AUAU E TAUTOKO ANA (AC/DC+):
| Diameter (mm) | 2.5 | 3.2 | 4.0 | 5.0 | |
| Roa (mm) | 350 | 350 | 400 | 400 | |
| Āpere | Papatahi | 55 – 85 | 90 – 130 | 130 – 180 | 180 – 240 |
| V me OH | 50 – 80 | 80 – 115 | 110 – 170 | 150 – 200 |
I runga i te piripono ki te ariā o te "kounga, ngā ratonga, te mahi me te tipu", kua riro mai i a mātou ngā whakawhirinaki me ngā whakamoemiti mai i ngā kaihoko o te whare me te ao whānui mō te hokohoko wera mō te Rhk 2.5mm 3.2mm 4.0mm 5.0mm Aws E7018 Waro Rino Āwhata Wera Hiko, ko tā mātou tumanako ka taea e mātou te whai hononga pai ki ngā kaipakihi o te ao katoa.
Hokonga Wera mōHaina E7018 Hiko Whakarewa me te Hiko Whakarewa E7018, E mihi ana mātou ki te whai wāhi ki te mahi pakihi ki a koe, ā, e tumanako ana mātou ki te tāpiri atu i ētahi atu taipitopito mō ā mātou hua me ā mātou otinga. Ka taea te whakamana i te kounga pai, te utu whakataetae, te tuku i te wā tika me te ratonga pono. Mō ētahi atu pātai, kaua e mangere ki te whakapiri mai ki a mātou.