Waea Whakarewa Nikara Konukōre ERNi-1 Nikara Tig Waea Whakakī Konganuku

Whakaahuatanga Poto:

E whakamahia ana te ER-Ni1 mō te whakarewa me te whakakikorua i ngā koranu Nickel 200 me Nickel 201.


Taipitopito Hua

Ngā Tohu Hua

Nikara KoranuWaea WhakarewaWaea TigERNi-1

Ngā Paerewa
EN ISO 18274 – Ni 2061 – NiTi3
AWS A5.14 – ER Ni-1

 

Ngā Āhuatanga me ngā Taupānga

E whakamahia ana te ER-Ni1 mō te whakarewa me te whakakikorua i ngā koranu Nickel 200 me Nickel 201.

He tino pai mō te hono i ngā koranu Monel me te parahi-nikarangā koranu ki ngā maitai waro.

He nui te titanium i roto i te Ni1 hei whakahaere i te pūngao o te konganuku whakarewa i roto i ngā tukanga whakarewa.

E whakamahia whānuitia ana i roto i ngā ahumahi tukatuka matū, te hanga muka hangai me ngā taputapu tukatuka kai, me ētahi atu.

 

Ngā Rauemi Tūāpapa Noa

Nikara 200 me te 201*
* He rārangi whakaahua, ehara i te rārangi katoa

 

% o te Hanganga Matū
C% Mn% Fe% P% S% Si%  
mōrahi mōrahi mōrahi mōrahi mōrahi mōrahi  
0.05 0.80 0.70 0.030 0.010 0.75  
             
Cu% Ni% Co% Ti% Al%    
mōrahi 93.00 mōrahi 2.00 mōrahi    
0.20 meneti 1.00 3.50 1.00    

 

Ngā Āhuatanga Mīhini
Kaha Kume ≥410 MPa  
Te Kaha o te Hua ≥200 MPa  
Te whakaroa ≥30 %  
Te Kaha o te Pānga ≥100 J  

He whakatau tata noa iho ngā āhuatanga ā-ringa, ā, ka rerekē pea i runga i te wera, te hau tiaki, ngā tawhā whakarewa me ētahi atu āhuatanga.

 

Ngā Hau Whakamarumaru

EN ISO 14175 – TIG: I1 (Argon)

 

Ngā Tūnga Whakarewa

EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG

 

Ngā Raraunga Tākai
Diameter Roa Taumaha  
1.60 mm

2.40 mm

1000 mm

1000 mm

5 kg

5 kg

 

 