Nikara KoranuWaea WhakarewaWaea TigERNiCrMo-10
| Ngā Paerewa |
| EN ISO 18274 – Ni 6022 – NiCr21Mo13Fe4W3 |
| AWS A5.14 – ER NiCrMo-10 |
Ngā Āhuatanga me ngā Taupānga
He koranu nikara-kōromium-molibdenum i hangaia mō te hono i te C22, 625, 825, ngā huinga rānei o ēnei koranu.
E whakarato ana i tētahi konganuku whakarewa kore-Nb pakari mō ngā whakarewa rerekē i roto i ngā maitai kore-waikura super austenitic me ngā maitai kore-waikura super duplex.
He ātete tino pai ki te ngatata o te ahotea me te waikura, te pirau o ngā poka me te waikura kapiti.
E whakamahia whānuitia ana mō ngā whakakikorua me ngā whakakikorua o ngā maitai koranu iti.
E whakamahia ana i roto i te whakarewanga o ngā pāpāho waikura kaha i roto i ngā tipu tukatuka matū, ngā paparanga ātete waikura me ngā taiao tai moana me ngā taiao hinu-matū kino, me ētahi atu.
Kei te ipurangi ngā Tiwhikete Whakamātautau @wilkinsonstar247.com
Ngā Rauemi Tūāpapa Noa
Koranu 22, Koranu 625, Koranu 825, Koranu 926*
* He rārangi whakaahua, ehara i te rārangi katoa
| % o te Hanganga Matū | ||||||
| C% | Mn% | Fe% | P% | S% | Si% | Cu% |
| mōrahi | mōrahi | 2.00 | mōrahi | mōrahi | mōrahi | mōrahi |
| 0.010 | 0.50 | 6.00 | 0.020 | 0.010 | 0.08 | 0.50 |
| Ni% | Co% | Cr% | Mō% | V% | W% | |
| 49.00 | mōrahi | 20.00 | 12.50 | mōrahi | 2.50 | |
| meneti | 2.50 | 22.50 | 14.50 | 0.30 | 3.50 | |
| Ngā Āhuatanga Mīhini | ||
| Kaha Kume | ≥690 MPa | |
| Te Kaha o te Hua | - | |
| Te whakaroa | - | |
| Te Kaha o te Pānga | - | |
He whakatau tata noa iho ngā āhuatanga ā-ringa, ā, ka rerekē pea i runga i te wera, te hau tiaki, ngā tawhā whakarewa me ētahi atu āhuatanga.
Ngā Hau Whakamarumaru
EN ISO 14175 – TIG: I1 (Argon)
Ngā Tūnga Whakarewa
EN ISO 6947 – PA, PB, PC, PD, PE, PF, PG
| Ngā Raraunga Tākai | |||
| Diameter | Roa | Taumaha | |
| 1.60 mm | |||
2.40 mm
3.20 mm1000 mm
1000 mm
1000 mm5 kg
5 kg
5 kg
Te Taunahatanga: Ahakoa kua whakapau kaha katoa kia tika ai ngā mōhiohio kei roto, ka taea te whakarerekē i ēnei mōhiohio me te kore panui, ā, ka taea anake te kī he mea tika mō te aratohu whānui.