AWS E430-16 Kowiri tira Hiko Hiko Kowirihanga Maamaa Nga Hiko Pee Korewha, He Kaituku Hoa Pai rawa atu.

Whakaahuatanga Poto:

Ko te G302 (AWS E430-16) he Cr17 kowiri tira hiko me te paninga titanium-konupora.Ka taea te whakamahi me te AC me te DC.


Taipitopito Hua

Tohu Hua

Kowiri tira fehokotaki'angaHikohiko

G302                                                  

GB/T E430-16

AWS E430-16 

Whakaahuatanga: Ko te G302 he Cr17 he kowiri tira hiko me te paninga titanium-calcium.Ka taea te whakamahi me te AC me te DC.

Taupānga: Ka whakamahia mo te whakapiri i te waikura-waikawa (waikawa nitric) me nga hanganga rino kowiri tira Cr17-wera.

 

Te hanganga matū o te whakarewa whakarewa(%):

C

Mn

Si

Cr

Ni

Mo

Cu

S

P

≤0.10

≤1.0

≤0.90

15.0 ~ 18.0

≤0.6

≤0.75

≤0.75

≤0.03

≤0.04

 

Nga ahuatanga miihini o te whakarewa whakarewa:

Tuemi whakamatautau

Te kaha tensile

Mpa

Te whakaroa

%

Ka whakamanahia

≥450

≥20

 

O nāianei e taunaki ana:

Te diameter o te tokotoko

(mm)

3.2

4.0

5.0

Waeherehere o naianei

(A)

80 ~ 120

100 ~ 160

150 ~ 200

 

Panui:

1. Me tunuhia te hiko mo te 1 haora i te taha o te 150 ℃ i mua i te mahi fehokotaki'anga;

2. Ko te wahi paiherea me whakamahana i mua i te 200°C i mua i te whakapiri.

 

Wenzhou Tianyu Electronic Co., Ltd. i whakapumautia i te tau 2000. Kua mahi matou ki te hanga ote hiko hikos, tokotoko fehokotaki'anga, apau i te fehokotaki'anganeke atu i te 20 tau.

Ko o tatou hua matua ko nga irahiko kowiri tira, ko nga hiko waro, ko nga hiko o te waro, ko te iti o te koranu, ko te whakarewa i nga hiko, ko te nickel & cobalt koranu hiko, ko te rino ngawari me te iti o te koranu, ko nga waea kowiri tira, ko nga waea hiko, ko nga waea hiko. waea fehokotaki'i konumohe, whao i raro i te pewa.waea, nickel & cobalt koranu waea fehokotaki'anga, parahi fehokotaki'anga waea, TIG & MIG waea fehokotaki'anga, tungsten electrodes, waro gouging electrodes, me etahi atu taputapu fehokotaki'anga & pau.

 