B-85 Te Hiko Whakawhitiwhiti Maamaa, Te Waa Whakawhitinga Mata, Te Rakau Waahi Pewa

Whakaahuatanga Poto:

Ko te paninga o tenei hiko he nui te chromium, na te mea he tino atete ki te kakahu na te kaha o te abrasion, te waku nui me te iti o te paanga, ahakoa i te teitei o te pāmahana me te hau kino.Kaua e pa ki te wiri nui, ki te pa ranei.


Taipitopito Hua

Tohu Hua

Te Hiko Rakau Rakau Maamaa

RECUBRIMIENTO KAITIaki

Momo Nama:B – 85

Te Taatari Metara Whakapumau (Uara angamaheni)

C

4.0%

Si

0.6%

Cr

35%

 

Āhuatanga:

Ko te paninga o tenei hiko he nui te chromium, na te mea he tino atete ki te kakahu na te kaha o te abrasion, te waku nui me te iti o te paanga, ahakoa i te teitei o te pāmahana me te hau kino.Kaua e pa ki te wiri nui, ki te pa ranei.

 

Ngā Āhuatanga Hangarau:Te pakeke mai i te 57 ki te 62 HRc.(E rua nga uhi)

 

Nāianei me te Polarity:

He pai ke atu i te naianei tauutuutu, te hiko ki te pou pai

ø mm.

1/8”

5/32”

3/16”

Amp.min.

120

170

220

Amp.max.

140

190

250

 

Nga tono:

• Kaikawe kaikawe koti

• Peere keri

• Nga niho whakamarumaru

• Puma keri

• Miihini keri

• Nga papu kirikiri

 

 

ROA: 350mm.

PAUNA mo ia pouaka: 20 kg/44 lbs.

 

 

Wenzhou Tianyu Electronic Co., Ltd. i whakapumautia i te tau 2000. Kua mahi matou ki te hanga ote hiko hikos, tokotoko fehokotaki'anga, me nga mea e pau ana mo te 20 tau neke atu.

Ko o tatou hua matua ko nga irahiko kowiri tira, ko nga hiko waro, ko nga hiko o te waro, ko te iti o te koranu, ko te whakarewa i nga hiko, ko te nickel & cobalt koranu hiko, ko te rino ngawari me te iti o te koranu, ko nga waea kowiri tira, ko nga waea hiko, ko nga waea hiko. waea fehokotaki'i konumohe, whao i raro i te pewa.waea, nickel & cobalt koranu waea fehokotaki'anga, parahi fehokotaki'anga waea, TIG & MIG waea fehokotaki'anga, tungsten electrodes, waro gouging electrodes, me etahi atu taputapu fehokotaki'anga & pau.

 

 

 

 