D256 (B-80) Irahiko Whakarewa Mata Pākeke, Tokotoko Whakarewa Papa, Rākau Whakarewa Āwhata

Whakaahuatanga Poto:

He hiko taketake e whakatakoto ana i te maitai konupora austenitic, ka whakapakeketia i te āhua matao, e tika ana mō ngā maitai o te hanganga kotahi me ngā wāhanga kua pāngia e te pānga kino me te karawarawa waenga.


Taipitopito Hua

Ngā Tohu Hua

Irahiko Rākau Whakarewa Mata MārōRODO P

RODO PARA RECUBRIMIENTO PROTECTOR

Momo Nama: D256 (B – 80)

Tātaritanga Konukura kua Whakatakotoria (Ngā uara noa)

C

1.2%

Mn

13.0%

Si

0.5%

Ni

3.0%

 

Ngā Āhuatanga:

He hiko taketake e whakatakoto ana i te maitai manganese austenitic, ka whakapakeketia e te huringa matao, e tika ana mō ngā maitai o te hanganga kotahi me ngā wāhanga i pāngia e te pānga kino me te pakū waenga. He mea tino pai mō te whakaora, te paninga me te whakatika i ngā wāhanga maitai Mn austenitic, ngā wāhanga me ngā wahi o ngā mīhini taumaha.

 

Ngā Āhuatanga Ā-ringa:Te pakeketanga 200-250 HB BRINELL i te wā i whakatakotoria ai, 300-400 HB Brinell

i muri i te whakapakeketanga o te mahi makariri.

 

Ngā Tūnga Whakarewa:Papatahi, Whakapae, Runga, Poutū ki Runga.

 

Iahiko me te Polarity:

Mō te au hurihuri, te au tika rānei

hiko ki te pou pai

ø mm

ø i roto

Āmipera

3.20

1/8

110-130

4.00

5/32

140-160

5.00

2/16

180-230

 

Ngā Whakamahinga: • Hei whakakī i ngā maitai konupora.

• Te hanga anō i ngā niho keri me ngā pākete.

• Ngā whitinga me ngā ngākau o ngā rēra.

• Ngā mira kohuke me ngā hama.

• Mā te patupatu ka piki ake tōna pakeke ki te 350 – 400 HB.

• I te wā e hanga hou ana, e pania ana rānei, whakamahia te AG AR-91 hei turanga.

• I ngā pāmahana neke atu i te 300 OC, ko ngā maitai Mn

Ka tīmata te ngoikore. E taunakihia ana kia mau ngā taura.

pekehia, te diameter me te amperage iti rawa e taea ana.

 

 

ROA: 350mm.

TAUHĀ MŌ IA POUAKA: 20 kg/44 lbs.

 

I whakatūria a Wenzhou Tianyu Electronic Co., Ltd. i te tau 2000. Kua uru mātou ki te hanga ohiko whakarewas, ngā tokotoko whakarewa, me ngā taputapu whakarewa mō ngā tau neke atu i te 20.

Ko ā mātou hua matua ko te kowiri tirahiko whakarewas, ngā irahiko whakarewa maitai waro, ngā irahiko whakarewa koranu iti, ngā irahiko whakarewa mata, ngā irahiko whakarewa koranu nikara me te koranu konumohe, ngā waea whakarewa maitai ngawari me te koranu iti, ngā waea whakarewa kowiri tira, ngā waea whakaheke hau-ārai, ngā waea whakarewa konumohe, ngā whakarewa pewa ruku. ngā waea, ngā waea whakarewa koranu nikara me te koranu konumohe, ngā waea whakarewa parahi, ngā waea whakarewa TIG me te MIG, ngā irahiko tungsten, ngā irahiko keri waro, me ētahi atu taputapu whakarewa me ngā taonga pau.

 

 

 

 