Kaihoko Taonga Whakatapua EM14KS Waea Waea Waea Waehere Wao, Wao Wao Rao mo te Waea Pewa Kua Rukuhia

Whakaahuatanga Poto:

Ko te EM14KS he mea whakarewa, he waro hiko hiko mo te pewa kua rukuhia.


Taipitopito Hua

Tohu Hua

Ko te EM14KS he mea whakarewa, he waro hiko hiko mo te pewa kua rukuhia.Ko te tikanga mo te whakapiri kotahi me te maha o te waro, me etahi koranu iti, he maitai i roto i nga tuunga awhi papatahi me te whakapae.Tīpakohia te EM14KS kei roto i nga taapiri iti o te titanium hei whakapai ake i te pakari o te whakarewa me te awhina ki te pupuri i te kaha i muri i te whakakore i te ahotea.Me whakamahi tenei irahiko mo te whakapiri pewa kua rukuhia anake.

WHAKARĀPOI:

EC1 ia AWS A5.17, SFA 5.17.

NGĀ KAUPAPA:

Tīpakohia te EM14KS i hoahoatia hei whakaputa i te matū putunga weld e rite ana ki tera i hangaia e te waea totoka, nga hiko EM14K.Ko te hoahoa waea karekau ka nui ake te reiti whakaheke i te waea totoka ina rere ana i te taumata o naianei.

Tīpakohia te EM14KS kia pai ake te whakahaere o te kuhu pirepire i te waea totoka.He whanui ake, he iti ake te ahua o te urunga o te hiko hiko, he iti ake te ahua o te wera i runga i nga paahi o te pakiaka, he ngoikore ranei nga hononga.

NGĀ TONO:

Tīpakohia te EM14KS he pai mo era tono e pa ana ki te whakapiri i nga oko pehanga me nga tira waro hanganga penei i te A36, A285, A515, me A516.Me whakamahi ki nga rerenga koretake ka taea te whakakapi ki nga waahi katoa he waea totoka, ka whakamahia te hiko EM14K.

TE WHAKAMAHI KAUPAPA KAUPAPA:

Wt%

C

Mn

P

S

Si

Ti

.06

1.55

.015

.015

.55

.05

NGĀ TAWHE WELDING E WHAKATAHIngia ana:

5/64”

Amps
250

Ngaohiko
26-27

WFS (ipm)
90

ESO (i roto)
¾”-1¼”

Te Retepe (pa/haora)
6.5

350

29-30

160

11

500

33-34

290

20

3/32”

275

28-29

80

1”-1¼”

8.5

450

32-33

155

15.5

600

37-38

245

24.7

1/8”

400

28-29

68

1”-1¼”

11.5

550

32-33

100

17

750

37-38

150

26.5

5/32”

425

30-31

45

1¼”-1½”

11.5

650

34-35

80

18.5

900

40-42

140

38


  • Tōmua:
  • Panuku: