Irahiko Whakarewa Mata Pākeke Irahiko Whakarewa Mata DIN 8555 (E10-UM-60-GRZ) mō te Whakarewa Āwhata

Whakaahuatanga Poto:

Ko te DIN 8555 (E10-UM-60-GRZ) he hikohiko SMAW whakaora-teitei kua pania taketake mō te papa mārō.


Taipitopito Hua

Ngā Tohu Hua

Te Whakarewatanga Mata MārōIrahiko

 

Paerewa: DIN 8555 (E10-UM-60-GRZ)

Momo Nama: TY-C LEDURIT 61

 

Whakatakotoranga me te Whakamahinga:

· He hikohiko SMAW whakaora teitei kua pania taketake mō te mata mārō.

· He mata tino mārō o ngā wāhanga e pāngia ana e te karawarawa nui me te pānga taurite.

· He pai mō ngā paparanga mārō whakamutunga i muri i te paparanga ārai.

· Ngā wāhanga o te tipu whakawerawera, ngā pae me ngā pereti kakahu, ngā pae waru, te oumu pupuhi, ngā pūnaha utu, ngā oumu sima, ngā niho me ngā ngutu peere, ngā mata.

 

Te hanganga matū o te konganuku kua whakatakotoria (%):

 

C

Si

Mn

Cr

Mo

Nb

W

V

Ni

Fe

DIN

He nui te ihirangi C me te ihirangi Cr

Para.

EN

1.5

4.5

-

0.5

3.0

25

40

-

4.0

-

-

-

-

4.0

Para.

Noa

3.2

1.0

1.8

29

-

-

-

-

-

Para.

 

 

Te pakeke o te konganuku kua whakatakotoria:

I te mea kua whakarewahia

(HRC)

1 paparanga i runga i te maitai me te C=0.15%

(HRC)

1 paparanga i runga i te maitai Mn teitei

(HRC)

60

55

52

 

Ngā Āhuatanga Whānui:

· Hanganga Moroiti Martensitic+Austenite+Carbides

· Te Hurihanga Mā te Mīhini anake

· Whakamaroketia anō mō ​​te 2 hāora i te 300℃ i mua i te whakamahinga.

 