Te Hiko Waahanga Maamaa DIN 8555 (E7-UM-250-KPR) Nga Rakau Werohanga Mata, Rakau Waahi Pewa

Whakaahuatanga Poto:

Ko te DIN 8555 (E7-UM-250-KPR) he hiko SMAW whakaora teitei kua pania.Te hanganga austenite katoa.He tino kaha te whakakaha mahi me te tino uaua.


Taipitopito Hua

Tohu Hua

Wehenga MaamaaHikohiko

 

Paerewa: DIN 8555 (E7-UM-250-KPR)

Momo Nama: TY-C BMC

 

Whakatakotoranga me te Taupānga:

· Whakakikoruatia taketake SMAW hiko whakaora teitei

· Te hanganga austenite katoa.He tino kaha te whakakaha mahi me te tino uaua.

· He pai mo te whakakakahu i runga i nga waahanga e pa ana ki te pehanga teitei me te wiri me te abrasion.Ka taea te hanga i te mata ki runga i te rino ferritic tae atu ki te austenitic maro Mn-rino ka taea te paiherea nga hononga o te Mn-maitai maro.

· Ko nga mara tono matua kei roto i te umanga maina me te raima, te whakawhiti tereina, nga papu dredge, nga piston hydraulic press, te waahanga kuru e pa ana ki te kohuke ngohengohe.

 

Te hanganga matū o te konganuku kua takoto (%):

 

C

Si

Mn

Cr

Ni

Mo

V

Fe

DIN

0.5

-

-

11.0

18.0

-

-

3.0

-

-

Bal.

EN

0.3

1.2

-

11.0

18.0

-

19.0

-

3.0

-

2.0

-

1.0

Bal.

Tikanga

0.6

0.8

16.5

13.5

-

-

-

Bal.

 

 

Te pakeke o te konganuku tuku:

As Welded

(HB)

Mahi-pakeke

(HB)

260

550

 

Āhuatanga whānui:

· Hangangaiti Austenite

· Mahinga Miihini anake

· Waahi Waahi.≤250 ℃

· Te whakamaroke Whero mo te 2 haora i te 300 ℃ i mua i te whakamahi.


  • Tōmua:
  • Panuku: