Tokotoko Whakarewa Rino Koranu Iti AWS E8018-G (J556Fe) Ngā Irahiko Ā-ringa mō te Pewa Whakarewa

Whakaahuatanga Poto:

He hiko rino koranu iti te J556Fe (AWS E8018-G) he paura rino, he paninga hauwai iti hoki. Ka taea te whakamahi i te AC me te DC, ā, ka taea te whakarewa i ngā tūranga katoa.


Taipitopito Hua

Ngā Tohu Hua

Irahiko Whakarewa Rino Koranu Iti

J556Fe                                              

GB/T E5518-G

AWS E8018-G 

Whakaahuatanga: He hiko rino koranu iti te J556fe, he paura rino, he paninga hauwai iti hoki. Ka taea te whakamahi i te AC me te DC, ā, ka taea te whakarewa i ngā tūranga katoa.

Whakamahinga: Whakamahia mō te whakarewa i te maitai waro reo me ngā hanganga maitai koranu iti pēnei i te Q390.

 

Te hanganga matū o te konganuku whakarewa (%):

C

Mn

Si

S

P

≤0.12

≥1.00

≤0.80

≤0.035

≤0.035

 

Ngā āhuatanga hangarau o te konganuku whakarewa:

tūemi whakamātautau

Te kaha o te kume

Mpa

Te kaha o te hua

Mpa

Te whakaroa

%

Uara pānga (J)

-40℃

Kua whakamanahia

≥540

≥440

≥17

≥27

 

Te nui o te hauwai horapa o te konganuku kua whakatakotoria: ≤10.0mL/100g (tikanga chromatography mercury, hau rānei)

Tirotiro hihi-X: tohu I

 

Iahiko e taunakitia ana:

(mm)

Te whānui o te tokotoko

2.5

3.2

4.0

5.0

(A)

Iahiko Whakarewa

70 ~ 110

100 ~ 140

140 ~ 170

190 ~ 240

 

Pānui:

1. Me tunu te hiko mō te 1 hāora i te 350℃ i mua i te mahi whakarewa;

2. He mea nui kia horoia te waikura, te unahi hinu, te wai, me ngā poke i runga i ngā wāhanga whakarewa i mua i te whakarewa;

3. Whakamahia te pewa poto i te wā e whakarewa ana. He tika te ara whakarewa whaiti.

 


  • O mua:
  • Panuku: