Te Hiko Waa Whakawhana Whakawhanake Iti AWS E7018-G Nga Waehere Raina Te Mana Rino me te Hauwai Iti

Whakaahuatanga Poto:

Ko te J507FeNi (AWS E7018-G) he hiko hiko koranu iti me te paura rino me te paninga hauwai iti.Ka taea te whakamahi mo nga waahi katoa me te AC me te DC


Taipitopito Hua

Tohu Hua

Iti Alloy Steel Welding Hiko

J507FeNi                                                    

GB/T E5018-G

AWS E7018-G

Whakaahuatanga: Ko te J507FeNi he hiko hiko koranu iti me te paura rino me te paninga hauwai iti.Ka taea te whakamahi mo nga waahi katoa me te AC me te DC.He iti ake te pumau o nga mahi o te whakahiatotanga AC ki tera o te raima DC

Taupānga: Whakamahia mō te fehokotaki'anga waro maitai me te iti pāmahana oko pēhanga maitai, pērā i 16MnDR, etc.

Te hanganga matū o te whakarewa whakarewa(%):

C

Mn

Si

Ni

S

P

≤0.08

0.80 ~ 1.30

≤0.65

1.20 ~ 2.00

≤0.030

≤0.030

 

Nga ahuatanga miihini o te whakarewa whakarewa:

Tuemi whakamatautau

 

Te kaha tensile

Mpa

 

Te kaha tuku

Mpa

 

Te whakaroa

%

 

Uara pānga (J)

-40 ℃

Ka whakamanahia

≥490

≥390

≥22

≥54

 

Ko te ihirangi hauwai whakamaoritanga o te konganuku penapena: ≤6.0mL/100g (tikanga glycerin)

Tirohanga X-ray: Ko taku tohu

 

O nāianei e taunaki ana:

Te diameter o te tokotoko
(mm)

3.2

4.0

5.0

Waeherehere o naianei

(A)

90 ~ 120

140 ~ 180

170 ~ 210

 

Panui:

1. Me tunu te electrode mo te 1 haora i te 350 ℃ i mua i te mahi fehokotaki'anga;

2. He mea nui ki te horoi i te waikura, te unahi hinu, te wai, me nga poke i runga i nga waahanga whakapiri i mua i te whakapiri.

 

Wenzhou Tianyu Electronic Co., Ltd. i whakapumautia i te tau 2000. Kua mahi matou ki te hanga ote hiko hikos, tokotoko fehokotaki'anga, me nga mea e pau ana mo te 20 tau neke atu.

Ko o tatou hua matua he kowiri tirate hiko hikos, waro maitai fehokotaki hiko hiko,iti koranu hiko fehokotaki'anga, te whakarewa i nga ira hiko, te nickel & cobalt koranu whakarewa hiko, te rino ngawari me te iti o te koranu waea, te kowiri tira waea, nga waea rewharewha kua parea te hau, nga waea konumohe konumohe, te pewa kua rukuhia.waea, nickel & cobalt koranu waea fehokotaki'anga, parahi fehokotaki'anga waea, TIG & MIG waea fehokotaki'anga, tungsten electrodes, waro gouging electrodes, me etahi atu taputapu fehokotaki'anga & pau.

 