Kowiri tira Waehere Waehere Pounamu AWS A5.4 E310H-16 Kaituku Hiko Hiko Kounga Kounga Pai

Whakaahuatanga Poto:

A432 (AWS A5.4 E310H-16) ko te 3Cr26Ni21 wera-ātete kowiri tira hiko me te titanium-konupora paninga.


Taipitopito Hua

Tohu Hua

Kowiri tira fehokotaki'angaHikohiko

A432                                 

GB/T E310H-16

AWS A5.4 E310H-16

Whakaahuatanga: A432 Ko te 3Cr26Ni21 te wera-aukati hiko hiko me te paninga titanium-calcium.Ka taea te whakamahi mo te AC me te DC me te mahi tino pai.He nui te kaha o te ngokingoki o te whakarewa, he pai te mahi tahi, me te iti o te kapiti waiariki.

Taupānga: Kei te tino whakamahia te reira mo te fehokotaki'anga HK40 maitai wera-ātete.

 

Te hanganga matū o te whakarewa whakarewa(%):

C

Cr

Ni

Mo

Mn

Si

Cu

S

P

0.35 ~ 0.45

25.0 ~ 28.0

20.0 ~ 22.5

≤0.75

1.0 ~ 2.5

≤0.75

≤0.75

≤0.030

≤0.030

 

Nga ahuatanga miihini o te whakarewa whakarewa:

Tuemi whakamatautau

 

Te kaha tensile

Mpa

Te whakaroa

%

Ka whakamanahia

≥620

≥10

 

O nāianei e taunaki ana:

Te diameter o te tokotoko

(mm)

3.2

4.0

5.0

Waeherehere o naianei

(A)

80 ~ 110

110 ~ 160

160 ~ 200

 

Panui:

  1. Me tunu te electrode mo te 1 haora i te 150 ℃ i mua i te mahi fehokotaki'anga;
  2. Na te mea he papaku te hohonutanga o te urunga i te wa e whakahiato ana i te AC, me whakamahi te mana hiko DC kia kaha ake ai te kuhu.kia kaua hoki e nui rawa te au ki te karo i te whero o te rakau whakapiri.

 

 

Wenzhou Tianyu Electronic Co., Ltd. i whakapumautia i te tau 2000. Kua mahi matou ki te hanga ote hiko hikos, tokotoko fehokotaki'anga, apau i te fehokotaki'anganeke atu i te 20 tau.

Ko o tatou hua matua he kowiri tirate hiko hikos, waro waro irihiko hiko fehokotaki'anga, iti koranu hiko fehokotaki'anga, mata fehokotaki'anga hiko, nickel & cobalt koranu hiko fehokotaki'anga, ngawari maitai & iti koranu waea fehokotaki'anga, kowiri tira waea fehokotaki'anga, hau-maarai rere rere i te taura waea, konumohe waea fehokotaki'anga, pewa wairere wairere .waea, nickel & cobalt koranu waea fehokotaki'anga, parahi fehokotaki'anga waea, TIG & MIG waea fehokotaki'anga, tungsten electrodes, waro gouging electrodes, me etahi atu taputapu fehokotaki'anga & pau.

 