AWS A5.4 E312-17 Kowiri tira Hiko Hiko Rakau Arc Rakau Welding Rods

Whakaahuatanga Poto:

Ko te AWS E312-17 he waahi-katoa me te tino rite ki te 312-16 engari ko te -17 paninga he nui ake te silica me te iti iho o te titani-um e hanga ana i te paanga "Spray-Arc" ina whakamahia ana ki runga i nga weera awhi whakapae.


Taipitopito Hua

Tohu Hua

Ko te AWS E312-17 he waahi-katoa me te tino rite ki te 312-16 engari ko te -17 paninga he nui ake te silica me te iti iho o te titani-um e hanga ana i te paanga "Spray-Arc" ina whakamahia ana ki runga i nga weera awhi whakapae.

whakarōpūtanga:

AWS A5.4 E312-17

ISO 3581-A E 29 9 R 1 2

WHAKAMAHI AWHINA

He rutile-taketake teitei CrNi-alloyed electrode tūnga katoa

He pai rawa mo te whakatika i te whakapiri

I tino whakawhanakehia mo nga tira uaua ki te wea, penei i nga pereti patu, austenitic Mn-maitai me nga C- maitai teitei.

He pai te weldability me te tuku whaiaro para

Weldable i runga i AC me DC+ polarity

Momo o naianei: DC/AC+

Te Hanga Matū o Inweld 312-17

Fe

C

Cr

Ni

Mo

Mn

Si

P

S

N

Cu

Taurite

0.15

28.0

8.0

0.75

0.5-2.5

0.90

0.04

0.03

---

0.75

-32.0

-10.5

Ko nga uara kotahi he morahi engari mena kua tohua.

Whakaahuatanga me nga tono

Ko te AWS E312-17 he waahi-katoa me te tino rite ki te 312-16 engari ko te -17 paninga he nui ake te silica me te iti ake o te titani-um e hanga ana i te paanga "Spray-Arc" ina whakamahia ana ki runga i nga weera awhi whakapae.Ka puta ano he putunga weld me te ahua ripple pai ake he papatahi ki te concave.Ko te 312-17 he puhoi ake te toi mīti, he pai ake te whakahaere ina whakamahi tikanga toia.He pai te kowhiringa mo nga tira uaua-ki-wela penei i te rino whakapakeke-rangi, te rino waro reo me te teitei.Ko te electrode tino pai ki te whakamahi i te waahi ko te whakarewa turanga he karaehe rino e kore e mohiotia.He pai mo te maha o nga tono rereke e pa ana ki te rino whakamaroke konupora, te rino patu, te maitai o te puna, te rino tereina, te rino nickel kakahu, te taputapu me te rino mate me te rino rererangi.Ka whakamahia noa hei paparanga-aukati-kaahua me te paparanga "buffer" i roto i nga tono uaua.Ka pakeke te mahi ki te 200 Brinell.Ko te 312-17 te teitei o te kaha me te kaha tuku o nga hiko kua whakakikoruatia he kowiri tira (kaore i whakauruhia).

Tawhā Manakohia

SMAW (DCEP – Hiko+)

Waea Diamita

Amperage

3/32”

50-80

1/8”

7-110

5/32”

100-140


  • Tōmua:
  • Panuku: