AWS E6013 (J421) Irahiko Whakarewa maitai waro, Ngā tokotoko whakarewa rutile

Whakaahuatanga Poto:

He hiko waro maitai te J421 (AWS E6013) he paninga titanium me te pāhare pākawa teitei. Ka taea te whakamahi mō te whakarewa i ngā tūranga katoa me te AC me te DC.


Taipitopito Hua

Ngā Tohu Hua

Te Whakarewatanga o te Rino WaroIrahiko

 J421                                                       

GB/T E4313

AWS A5.1 E6013

Whakaahuatanga: He hiko waro maitai te J421, he paninga titanium me te pāhare pākawa waro teitei. Ka taea te whakamahi mō te whakarewa i ngā tūranga katoa me te AC me te DC. He tino pai te mahi whakarewa, ā, he ngāwari ki te tīmata anō i te pewa.

Taupānga: He pai mō te whakarewa i ngā hanganga maitai waro-iti, he tino pai mō te whakarewa wā poto o ngā wahi iti o ngā pereti angiangi me ngā whakarewa poto me te whakarewa hipoki e hiahia ana ki ngā mata maeneene.

 

Te hanganga matū o te konganuku whakarewa (%):

C

Mn

Si

S

P

≤0.12

0.30~0.60

≤0.30

≤0.035

≤0.040

 

Ngā āhuatanga hangarau o te konganuku whakarewa:

tūemi whakamātautau

Te kaha o te kume

Mpa

Te kaha o te hua

Mpa

Te whakaroa

%

Uara pānga (J)

Te Mahana Noa.

0℃

Kua whakamanahia

≥420

≥330

≥17

—

—

Kua whakamatauria

460 ~ 540

≥340

18 ~ 26

50 ~ 75

≥47

Tirotiro hihi-X: taumata II

Iahiko e taunakitia ana:

Te whānui o te tokotoko

(mm)

2.0

2.5

3.2

4.0

5.0

5.8

Iahiko whakarewa

(A)

40 ~ 70

50 ~ 80

80 ~ 120

150 ~ 190

180 ~ 240

220 ~ 280

 

I whakatūria a Wenzhou Tianyu Electronic Co., Ltd. i te tau 2000. Kua uru mātou ki te hanga ohiko whakarewangā rakau whakarewa, me ngā taonga whakarewa mō ngā tau neke atu i te 20.

Ko ā mātou hua matua ko te kowiri tirahiko whakarewas, ngā irahiko whakarewa maitai waro, ngā irahiko whakarewa koranu iti, ngā irahiko whakarewa mata, ngā irahiko whakarewa koranu nikara me te koranu konumohe, ngā waea whakarewa maitai ngawari me te koranu iti, ngā waea whakarewa kowiri tira, ngā waea whakaheke hau-ārai, ngā waea whakarewa konumohe, ngā whakarewa pewa ruku. ngā waea, ngā waea whakarewa koranu nikara me te koranu konumohe, ngā waea whakarewa parahi, ngā waea whakarewa TIG me te MIG, ngā irahiko tungsten, ngā irahiko keri waro, me ētahi atu taputapu whakarewa me ngā taonga pau.

 