Irahiko maitai waro hauwai iti E6011

Whakaahuatanga Poto:

AWS E6011hiko whakarewahe momo pāhare pākawa cellulose, e whakamahia ana mō te whakarewa poutū ki raro. Mō te whakarewa AC me te whakarewa DC.


Taipitopito Hua

Ngā Tohu Hua

Tono
He pai ngā rakau whakarewa AWS E6011 mō te whakarewa i ngā hanganga oko pēnei i ngā whare me ngā piriti, ngā tāke rokiroki, ngā paipa me ngā hononga oko pēhanga.

AWS E6011hiko whakarewaHe momo pāhare pākawa cellulose tēnei, e whakamahia ana mō te whakarewa poutū ki raro. Mō te whakarewa AC me te whakarewa DC. E whakamahi ana i ngā hangarau matatau o tāwāhi, ā, he tino pai ngā āhuatanga hangarau whakarewa. Me whakahaere te roa o te ARC i roto i te whānuitanga whaitake. Kāore e tika ana mō te whakarewa paparanga maha me te whakarewa hipoki.

Te Hanganga Matū (%)
C Mn Si S P
≤0.2 0.3-0.6 ≤0.22 ≤0.03 ≤0.04
Ngā Āhuatanga Hangarau o te Konukura Kua Whakatakotoria
Tuemi Whakamātautau Rm (N/mm2) Rel (N/mm2) A (%) KV2(J) 0℃
Uara Pūtāhui ≥420 ≥330 ≥22 ≥47
Hua Whānui 485 380 24 86
Iahiko Tohutoro (DC)
Diameter φ2.0 φ2.5 φ3.2 φ4.0 φ5.0
Āmipera 40 ~ 70 50 ~ 90 90 ~ 130 130 ~ 210 170 ~ 230

TE MOMO O TE AU: Au Tika, Auhiko Pai (DCEP) AC rānei

NGĀ TIKANGA WHAKAPĀNGA E TAUTOKO ANA:

Te Roa o te Āwhata – Te roa toharite (1/8” ki te 1/4”)

Papatahi – Me noho ki mua i te puna wai, me te whakamahi i te nekehanga whiu mārie

Whakapae – Whakapikohia te hikohiko ki te pereti o runga kia paku angiangi

Poutū ki Runga – Tikanga whiu, raranga rānei

Poutū ki raro – Whakamahia he amperage teitei ake me te tere haere, me te noho ki mua i te puna wai

I runga ake – Me noho ki mua i te puna wai, me te whakamahi i te nekehanga whiu mārie

Whakarongo:
1. He māmā noa te pā ki te makuku, me waiho kia maroke.
2. Me whakamahana ina pakaru te putea, ina mimiti rānei te makuku, me noho te pāmahana whakamahana i waenga i te 70C ki te 80C, me noho te wā whakamahana i waenga i te 0.5 ki te 1 hāora.
3. Mēnā kei te whakamahi koe i ngā irahiko whakarewa 5.0mm, he pai ake te whakamahi i ngā hiko pana-teitei, iahiko-iti, hei whakapai ake i te mahi whakarewa.