AWS ENiCrFe-4 Nickel Alloy Welding Electrodes mo te Wehenga Pouaka Whakaara, Nga Waehere Paerewa

Whakaahuatanga Poto:

Ko te Ni307-4 (AWS ENiCrFe-4) he hikohiko-nikeli me te paninga konutai iti-waiwai.Whakamahia te DCEP (te hiko tika o naianei pai).


Taipitopito Hua

Tohu Hua

Nickel meNickel Alloy Welding Electrode

Ni307-4                                                     

GB/T ENi6093

AWS A5.11 ENiCrFe-4

 

Whakaahuatanga: Ko te Ni307-4 he electrode i runga i te nickel me te paninga konutai iti-hydrogen.Whakamahia te DCEP (direct current electrodepai).He pai rawa te mahi fehokotaki'anga me te mura o te arc, he iti ake te mokamoka, he ngawari te tango para,

me te paihere ataahua.

 

Taupānga: Kei te whakamahia mo te whakapiringa o nga koranu nickel-chromium-rino, penei i te Ni600, Ni800 / 800H me nga superalloys rite, nickel-based superalloys ranei me te wera mahi o 900 ° C. Ka taea hoki te whakamahi mo nga tira iti-mahana kei roto. Ni3% ~ 9%, penei i te ASTM A333, A334, A353, A522, Ka taea hoki te whakamahi i te whakarewatanga o te A553 mo te whakarewa whakarewa rereke i waenganui i Mo400, Ni825, he kowiri tira me te rino koranu iti.

 

Te hanganga matū o te whakarewa whakarewa(%):

C

Mn

Fe

Si

Ni

Cr

Mo

Nb + Ta

S

P

≤0.20

1.0 ~ 5.0

≤12.0

≤1.0

≥60.0

13.0 ~ 17.0

1.0 ~ 3.5

1.0 ~ 3.5

≤0.015

≤0.020

 

Nga ahuatanga miihini o te whakarewa whakarewa:

Tuemi whakamatautau

Te kaha tensile

Mpa

Te kaha tuku

Mpa

Te whakaroa

%

Ka whakamanahia

≥650

≥360

≥18

 

O nāianei e taunaki ana:

Te diameter o te tokotoko

(mm)

2.5

3.2

4.0

Waehere naianei

(A)

60 ~ 90

80 ~ 110

110 ~ 150

 

Panui:

1. Me tunuhia te electrode mo te 1 haora i te taha o te 300 ℃ i mua i te mahi fehokotaki'anga;

2. He mea nui ki te horoi i te waikura, te hinu, te wai, me nga poke i runga i nga waahanga whakapiri i mua i te whakapiri.Ngana ki te whakamahi i te pewa poto ki te wea.

 

 