Ngā Irahiko ENiCrFe-3 mō te Nikara

Whakaahuatanga Poto:

Kei te whakatakoto te irahiko i te konganuku whakarewa 65Ni-20Cr-2Nb-1.5Mo.


Taipitopito Hua

Ngā Tohu Hua

WAEHERE EN ISO: 14172:ENi6082

Kei te whakatakoto te irahiko i te konganuku whakarewa 65Ni-20Cr-2Nb-1.5Mo. He konganuku whakarewa kounga-irahiko me ngā āhuatanga pai rawa atu. He mea tino pai mō te whakarewa i ngā koranu o ngā hanganga rite ki a rātou anō, mō te mata o te maitai ki te koranu Nickel-Chromium-Rino ina kore he kino o ngā ihirangi Manganese teitei, mō te whakarewa i te taha kua whakakikoruatia o te maitai Nickel Chromium-Rino me ngā huinga konganuku rerekē. He pai mō te whakakikorua i ngā pereti whakarewa. He mea tino taunaki mō te whakarewa i ngā maitai Ni 9% mō te mahi cryogenic. Ka whakamahia hoki mō te whakarewa i ngā koranu Nickel-Chromium e whakamahia ana mō ngā tono pāmahana teitei pēnei i ngā huānga whakamahana oumu me ngā ngongo whakahou.

TE HANGANGA MATUA NOA O NGĀ MEKANI WHAKAPĀ KATOA

Huānga C Mn Si Cr Ni Fe Nb Cu Ti S P
Ōrau ≤0.10 5.0-9.5 ≤1.0 13.0-17.0 ≥59.0 ≤10.0 1.0-2.5 ≤0.50 ≤1.0 ≤0.015 ≤0.030

NGĀ ĀHUATANGA MĪHINI NOA O NGĀ MEKANI WHAKAPĀ KATOA

UTS YS Te whakaroa Kaha Pānga CVN (J) Whānuitanga Taha Te Kaha Ngoki i
(MPa) (MPa) (L= 5d)% i te iti iho i te 196°C i te iti iho i te 196°C (mm) 600°C mō ngā hāora 1000.
620 500 30 75 0.85 160 MPa

NGĀ RARAUnga O NĀIANEI ME NGĀ RARAUnga TAKAI: DC (+)

Rahi (mm)

Dia x Roa

5×350

4×350

3.15×350

2.5×350

Awhe o Ia Wā (Amps)

150-180

120-150

80-110

60-70

Taumaha/Pouaka (kgs)

2.5

2.5

2.5

2.5

Te Whakatūpato

1. Kia maroke ngā irahiko. Whakamaroketia anō ngā irahiko i te 300-325°C mō te haora kotahi.

2. Kia poto te pewa, kia poto te poroporo aho, kia iti hoki te wera e uru mai ana.

3. Tukua te whakarewa kia whakamatao ki raro iho i te 50 C i mua i te whakatakoto i te paparanga e whai ake nei.


  • O mua: