E308-16 hiko whakarewa maitai kore waikura

Whakaahuatanga Poto:

Irahiko Whakarewa Kowiri tiraHe hiko whakarewa momo titanium raina te E308-16 mō te maitai kore waikura waro-iti rawa.


  • :
  • Taipitopito Hua

    Ngā Tohu Hua

    AWS:Hiraka Whakarewa Kowiri tira SFA 5.4 E308-16

    He momo titanium raina te E308-16hiko whakarewamō te maitai kore waikura waro-iti rawa.

    Whakarōpūtanga:

    AWS A5.4 / ASME SFA5.4 E308-16

    JIS Z3221 D308-16

    Whakaahuatanga:

    Ko te Hiko Whakarewa Kowiri tira E308-16 he momo titanium rainahiko whakarewamō te maitai kore waikura waro-iti rawa. He tino pai ngā āhuatanga miihini o te konganuku whakarewa, ā, he pai te ātete ki te waikura intergranular nā te mea he ≤. 0.04% b te ihirangi waro kei roto. Ka taea te whakamahi mō ngā tūranga whakarewa katoa me te mahi tino pai: he pewa pumau, he iti ngā tauhiuhi, he pai te āhua o te whakarewa. Ā, he pai te ātete wera o te hiko whakarewa, kāore e ngawari ki te whero, ā, kāore e puta he porosity hau.

    Taupānga:

    Te whakarewanga o te maitai 18%Cr-8%Ni.

    He pai mō ngā hanganga whakarewa i hangaia mai i te maitai kore waikura waro iti rawa 022Cr-19Ni10, pērā i te muka hangai, te tongi,

    ngā taputapu matū hinu, me ētahi atu

     

    Te Hanganga Matū o te Konukura Kua Whakatakotoria (E308L-16) (%)

    Taonga C Mn Si Cr Ni S P Cu Mo
    uara paerewa ≤0.08 0.5-2.5 ≤0.90 18.0-21.0 9.0-11.0 ≤0.030 ≤0.040 ≤0.75 ≤0.75
    Uara tauira 0.043 1.10 0.78 19.52 9.76 0.012 0.031 0.02 0.032

    Ngā Āhuatanga Hangarau o te Konganuku Kua Whakatakotoria (%)

    Me whakatau te mahi ārai-waikura me te hanganga ferrite i waenga i te kaihoko me te kaihoko.

    Taonga Kaha Kume (MPa) Te roa (%)
    uara paerewa ≥550 ≥25
    Uara tauira 601 41

    Ngā tono

    Ka whakamahia hei whakarewa i te momo hanganga maitai kowiri tira ātete wera kotahi e mahi ana i te pāmahana teitei, ka taea hoki te whakamahi hei whakarewa i te maitai chrome sclerosing nui (pēnei i te Cr15Mo, Cr9Mo, Cr13, Cr28) me ngā maitai rerekē.

    Diameter (mm)

    2.0

    2.5

    3.2

    4.0

    5.0

    Iahiko Whakarewa (A)

    25-50

    50-80

    80-110

    110-160

    160-200

    Iahiko: AC, DC+ rānei

    Ngā Tuhipoka mō te Whakamahinga:

    1. Kia poto te pewa.

    2. Tangohia ngā paru pērā i te hinu me te puehu i te awaawa.

    3. Whakamarokehia ngā hiko i te 350 (662) mō te 60 meneti i mua i te whakamahinga

     


  • O mua:
  • Panuku: