Ko Tyue Brand AWS ENiCrMo-4 Nickel and Nickel Based Alloy Welding Electrode, Pai rawa atu i te Arc Welding Rods, Kaihokohoko Welding

Whakaahuatanga Poto:

Ko te Ni327-4 (ENiCrMo-4) he hikohiko nickel-based me te paninga konutai iti-hydrogen.Whakamahia te DCEP (te hiko tika o naianei pai).


Taipitopito Hua

Tohu Hua

Nickel and Nickel Alloy Welding Electrode

Ni327-4                                                     

GB/T ENi6276

AWS A5.11 ENiCrMo-4

 

Whakaahuatanga: Ko te Ni327-4 he electrode-nikeli me te paninga konutai iti-hydrogen.Whakamahia te DCEP (direct current electrodepai).He pai rawa te mahi fehokotaki'anga me te mura o te arc, he iti ake te mokamoka, he ngawari te tango para,

me te paihere ataahua.Ko nga ahuatanga miihini o te konganuku kua penapena he pumau.

 

Taupānga: Ka whakamahia mo te whakapiri i nga koranu nickel-chromium-molybdenum iti-carbon, penei i te Hastelloy C276, ASTM B574, B575, B619, B622, B626, a ka taea hoki te whakamahi mo te whakapiri i nga tira rereke me etahi atu koranu nickel-based.

 

Te hanganga matū o te whakarewa whakarewa(%):

C

Mn

Si

Cr

Ni

Mo

≤0.02

≤1.0

≤0.2

14.5 ~ 16.5

≥50.0

15.0 ~ 17.0

W

Co

Fe

S

P

Ētahi atu

3.0 ~ 4.5

≤2.5

4.0 ~ 7.0

≤0.015

≤0.020

≤0.5

 

Nga ahuatanga miihini o te whakarewa whakarewa:

Tuemi whakamatautau

Te kaha tensile

Mpa

Te kaha tuku

Mpa

Te whakaroa

%

Ka whakamanahia

≥690

≥400

≥22

 

O nāianei e taunaki ana:

Te diameter o te tokotoko

(mm)

2.5

3.2

4.0

Waehere naianei

(A)

60 ~ 90

70 ~ 110

90 ~ 150

 

Panui:

1. Me tunu te electrode mo te 1 haora i te 300 ℃ i mua i te mahi fehokotaki.Ngana ki te whakamahi i te pewa poto ki te wea;

2. He mea nui ki te horoi i te waikura, te hinu, te wai, me nga poke i runga i nga waahanga whakapiri i mua i te whakapiri.

3. Whakamātauria ki te whakamahi i te pūngao raina iti ina fehokotaki'anga, maha-apa me te maha-haere fehokotaki'anga.

 