Irahiko whakarewa E410NiMo-15

Whakaahuatanga Poto:

Ko te E410NiMo-15 he hiko whakarewa maitai kore waikura martensitic me te paninga konutai hauwai-iti 11.0-12.5% ​​Cr, 4.0-5.0 Ni, me te 0.40-0.70% Mo.


Taipitopito Hua

Ngā Tohu Hua

Paerewa e rite ana

GB/T 983-2012 E410NiMo-15

AWS A5.4M-2012 E410NiMo-15

Rauemi ōrite:1.4317 GX4CrNi13-4,1.4313 X3CrNiMo13-4,1.4407 GX5CrNiMo13-4,1.4414 GX4CrNiMo13-4,ACI Gr. CA6NM,UNS S41500

Whakaahuatanga

Ko te E410NiMo-15 he hiko whakarewa maitai kore waikura martensitic me te paninga konutai hauwai-iti, kei roto ko te 11.0-12.5% ​​Cr, 4.0-5.0% Ni, me te 0.40-0.70% Mo. He pai mō te whakarewa pewa whakarewa pareparenga katoa-tūnga (SMAW) me te pewa pumau, te iti o te tauhiuhi, me te wetewete pai o te para. He kaha teitei te whakarewa kua whakatakotoria, he ātete pai ki te waikura, me te ātete ki te pakaru. E taunakihia ana te whakamahana mua mō ngā wahi mahi matotoru, ā, me whai maimoatanga wera muri-whakarewa (PWHT) i te 580~620℃ (1-2 hāora, whakamatao hau, AC).

Tono

He pai mō te whakarewa i te maitai whakarewa ASTM CA6NM, ngā maitai raupapa 13%Cr-4%Ni (hei tauira, Cr13Ni4Mo, Cr13Ni5Mo), me ngā maitai kowiri tira martensitic rite tonu. Ko ngā tono noa ko te whakatikatika i te whakarewa o ngā kaitahuri hiko wai, ngā tinana takirere, ngā paipa pēhanga teitei, me te mata o ngā wāhanga kua mau i te cavitation. Ka whakamahia hoki mō te whakatikatika i te mata mārō o ngā wāhanga ātete-kakahu pērā i ngā roera kuru me ngā anga papu.

Te Hanganga Matū o te Mea Whakarewa (%)

Huānga C Mn Si P S Cr Ni Mo Cu
Whakaritenga ≤0.06 ≤1.0 ≤0.90 ≤0.04 ≤0.03 11.0-12.5 4.0-5.0 0.40-0.70 ≤0.75
Hua Whakamātautau 0.029 0.7 0.32 0.028 0.01 12.26 4.50 0.55 0.01

Ngā Āhuatanga Hangarau o te Konukura Kua Whakatakotoria

Ingoa Whakamātautau Kaha Kume (Mpa) Te roanga% hihi-X Whakamātautau Pānga,(+20℃)J Te pakeketanga HB Hauwai Marara (ml/100g)
Whakaritenga ≥760 ≥15 Taumata Tuatahi – – ≤5
Hua Whakamātautau 845 19 Taumata Tuatahi 60-90 250-310 ≤5

Ngā Tawhā Whakarewa i Manakohia

Pūtake Mana: Rāhui DC (DC-)

nāianei i tūtohutia

Diameter o te tokotoko (mm) 3.2 4.0 5.0
Iahiko Whakarewa (A) 80-120 120-160 150-190

Pānui:

1. Tunua te hiko i te 300℃ mō te haora i mua i te whakamahinga hei tango i te makuku.
2. Horoia te waikura, te hinu, me te makuku mai i te mata o te konganuku turanga; whakamahia te mahi pewa poto mō ngā pīrere whakarewa whaiti.
3. Me mahi tonu te PWHT i muri i te whakarewanga hei karo i te pakarukaru.

  • O mua: