Whakaahuatanga Poto:

He waea maitai kore waikura martensitic te EC410NiMo, he mea hanga ki te hau, ā, kei roto i te hanganga matū ko te 11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, me te 0.40 – 0.70% Mo.

Taipitopito Hua

Ngā Tohu Hua

Paerewa e rite ana

GB/T 17853-2018 TS410NiMo-FC11

AWS A5.22M-2012 E410NiMoT1-1

Rauemi ōrite: 13Cr-4Ni (EN1.4313/UNS S41500)

Whakaahuatanga

He waea maitai kore waikura martensitic te EC410NiMo, he mea hanga ki te hauhautanga, ā, kei roto i te hanganga matū ko te 11.0 – 12.5% ​​Cr, 4.0 – 5.0% Ni, me te 0.40 – 0.70% Mo. He pai mō ngā tūranga katoa.whakarewa pewa āwhata-whakarerekē(FCAW) me te pewa pumau, te iti o te tauhiuhi, me te tino pai o te wetewete i te para. He pai te ātete ki te kakahu, te ātete ki te pakaru, me ngā āhuatanga miihini o te konganuku kua whakatakotoria. E taunakihia ana kia whakamahanahia i mua i te 150 – 260℃, ā, me whakamahana i muri i te whakarewanga (PWHT) i te 590~620℃ mō te 1 hāora (ā, muri iho ka whakamataohia te hau, AC) i muri i te whakarewanga.

Tono

He mea tino pai mō te whakarewa i te maitai whakarewa ASTM CA6NM me ngā maitai raupapa 13%Cr – 4%Ni. Whakamahia mō te whakatika i ngā mata mārō o ngā reera kerēni, ngā roera tā, ngā toki maitai, ngā wāhanga hiko wai kua mau i te cavitation, me ngā wāhanga hanganga e hiahia ana ki te ātete ki te waikura me te kakahu.

Te Hanganga Matū o te Mea Whakarewa (%)

Huānga C Cr Ni Mo Mn Si P S Cu
Whakaritenga ≤0.06 11.0-12.5 4.0-5.0 0.40-0.70 ≤1.00 ≤1.00 ≤0.040 ≤0.030 ≤0.75
Hua Whakamātautau 0.02 12.3 4.65 0.54 0.59 0.33 0.023 0.01 0.01

Ngā Āhuatanga Hangarau o te Konukura Kua Whakatakotoria

Ingoa Whakamātautau Kaha Kume (MPa) Te roanga% hihi-X Whakamātautau Pānga (+20℃)J Te pakeketanga HB Hauwai Marara (ml/100g)
Whakaritenga ≥760 ≥15 Taumata Tuatahi – – ≤5
Hua Whakamātautau 845 19 Taumata Tuatahi 60-90 250-310 ≤5

 

Tawhā Whakarewa i Manakohia

Pūtake Mana: DC Whakamuri (DC-)

Te Diameter Waea me te Iahiko:

Iaianei e Manakohia ana:

Diameter o te tokotoko (mm) 3.2 4.0 5.0
Iahiko Whakarewa (A) 80-120 120-160 150-190

Pānui

1. Tunua te hiko i te 300℃ mō te haora i mua i te whakamahinga hei tango i te makuku.

2. Horoia te waikura, te hinu, me te makuku mai i te mata o te konganuku turanga; whakamahia te mahi pewa poto mō ngā pīrere whakarewa whaiti.

3. Me mahi tonu te PWHT i muri i te whakarewanga hei karo i te pakarukaru.

 

 