Irahiko whakarewa maitai waro E6010

Whakaahuatanga Poto:

He momo hiko konutai rutile-cellulosic te E6010.


Taipitopito Hua

Ngā Tohu Hua

AWS E6010 Irahiko Whakarewa Rino Ngāwari

NGĀ TONO:

He pai mō te whakarewa i ngā hanganga maitai waro-iti pērā i te paipa, te hanga kaipuke me te piriti me ētahi atu.

NGĀ WHAKARĀPOPOTONGA:

AWS A5.1 / ASME SFA5.1 E6010

JIS Z3211 D4310

NGĀ ĀHUATANGA:

He momo hiko konutai rutile-cellulosic te E6010. Ka taea te whakarewa mō ngā tūranga katoa (ina koa mō te tūranga poutū-ki-raro) me te DC+ anake. He tino pai te mahi whakarewa hei pewa pumau, he iti te tauhiuhi, he ngāwari te tango para me te kaha ki te tahu. He pai ake te whakahaere i te puna rewa, he kaha ake te kaha o te pewa me te hohonu ake o te urunga i te tūranga poutū-ki-raro.

TE HANGA MATUA O NGĀ MEA WHAKAPĀ KATOA: (TAU MĀ %)

Ngā taonga C Mn Si S P Ni Cr Mo V
Ngā Whakaritenga ≤0.20 0.3-0.6 ≤0.30 ≤0.035 ≤0.040 ≤0.30 ≤0.20 ≤0.30 ≤0.08
Ngā Hua Noa 0.09 0.48 0.23 0.020 0.025 0.030 0.035 0.005 0.004

NGĀ ĀHUATANGA MĪHINI O NGĀ MEKANI WHAKAPĀ KATOA:

Ngā taonga Rm/MPa Rel/Rp0.2 /MPa A/% KV2 (-30℃) /J
Ngā Whakaritenga ≥430 ≥330 ≥20 ≥27
Ngā Hua Noa 475 400 26 80

WHAKATŪPATO:

1. I te nuinga o te wā, kāore e hiahiatia kia whakamarokehia anō te hiko i mua i te whakarewanga. Mēnā ka pāngia e te haukū, me whakamaroke anō i te 70℃-90℃ mō te 1 hāora.

2. Me tango te waikura, te hinu, te wai me ērā atu poke o te wāhi whakarewa i mua i te whakarewatanga.

NGĀ TIKANGA WHAKAHAERE NOA: ( DC+)

Diameter (mm) 2.5 3.2 4.0 5.0
Roa (mm) 300 350 400 400
Iaianei (A) 50-80 60-100 100-140 140-180

TE TĀKAI:

5kg/pouaka, 4 pouaka/kātene, 20kg/kātene, 50 kātene/pallet. 21MT -26MT ia 1X20″ FCL.

 

OEM/ODM:

E tautoko ana mātou i te OEM/ODM, ā, ka taea e mātou te hanga i ngā takai kia rite ki tāu hoahoa, tēnā whakapā mai ki a mātou mō ngā kōrero taipitopito.

 

Ngā Āhuatanga o te Whakamahinga:

He pewa tino pumau.

He tino kaha ki te tango i te para.

He papaku te urunga.

He ātete pai ki te wera me te waikura.

He ātete pai rawa atu ki te pakaru.