Ni327-6 Nickel Alloy Welding Electrodes AWS A5.11 ENiCrMo-6 Welding Rods, Welding Structural Arc Welding Stick Electrodes

Whakaahuatanga Poto:

Ko te Ni327 -6 (AWS A5.11 ENiCrMo-6) he hikohiko nickel-based me te iti-hydrogen sodium coating.Whakamahia te DCEP (te hiko tika o naianei pai).


Taipitopito Hua

Tohu Hua

Nickel and Nickel Alloy Welding Electrode

Ni327-6                                                     

GB/T ENi6620

AWS A5.11 ENiCrMo-6

Whakaahuatanga: Ko te Ni327 -6 he electrode nickel-based me te iti-hydrogen sodium coating.Whakamahia te DCEP (direct current electrodepai).He pai rawa te kirihou, te pakari me te kapiti o te konganuku kua penapena.Ko te konganuku kua penapena he whakarea roha rarangi rite ki tera o te maitai, he kaha te kaha me te kaha o te waikura i te pāmahana rūma me te pāmahana teitei.

Taupānga: Kei te whakamahia te reira mo te fehokotaki'anga o Ni9% maitai, a ka taea hoki te whakamahi mo te fehokotaki'anga o maitai rerekē me koranu uaua-ki-weld.

 

Te hanganga matū o te whakarewa whakarewa(%):

C

Mn

Si

Ni

Mo

Fe

Cu

≤0.10

2.0 ~ 4.0

≤1.0

≥55.0

5.0 ~ 9.0

≤10.0

≤0.5

Nb + Ta

W

Cr

S

P

Ētahi atu

 

0.5 ~ 2.0

1.0 ~ 2.0

12.0 ~ 17.0

≤0.015

≤0.020

≤0.5

 

 

Nga ahuatanga miihini o te whakarewa whakarewa:

Tuemi whakamatautau

Te kaha tensile

Mpa

Te kaha tuku

Mpa

Te whakaroa

%

Ka whakamanahia

≥620

≥350

≥32

 

O nāianei e taunaki ana:

Te diameter o te tokotoko

(mm)

2.5

3.2

4.0

Waehere naianei

(A)

50 ~ 70

80 ~ 100

110 ~ 150

 

Panui:

1. Me tunu te electrode mo te 1 haora i te 300 ℃ i mua i te mahi fehokotaki.Ngana ki te whakamahi i te pewa poto ki te wea;

2. He mea nui ki te horoi i te waikura, te hinu, te wai, me nga poke i runga i nga waahanga whakapiri i mua i te whakapiri.

3. Whakamātauria ki te whakamahi i te pūngao raina iti ina fehokotaki'anga, maha-apa me te maha-haere fehokotaki'anga.

 

 