Ngā Irahiko Whakarewa Koranu Nikara Ni327-3, AWS A5.11 ENiCrMo-3 Rakau Nikara mō te Whakarewa Āwhata, Kaiwhakarato Rauemi Whakarewa Pai rawa atu

Whakaahuatanga Poto:

Ko te Ni327 -3 (AWS ENiCrMo-3) he irahiko nikara me te paninga konutai hauwai-iti. Whakamahia te DCEP (irahiko au tika). He tino pai te kirihou, te pakari me te ātete ki te pakaru o te konganuku kua whakatakotoria, ā, he kaha teitei me te ātete ki te waikura i te pāmahana rūma me te pāmahana teitei.


Taipitopito Hua

Ngā Tohu Hua

Nikara me te Nikara KoranuWhakarewaIrahiko

Ni327-3                                                     

GB/T ENi6625

AWS A5.11 ENiCrMo-3        

Whakaahuatanga: Ko te Ni327 -3 he irahiko e hangai ana ki te nikara me te paninga konutai hauwai-iti. Whakamahia te DCEP (irahiko iahiko tika)(pai). He tino pai te kirihou, te pakari me te ātete ki te pakaru o te konganuku kua whakatakotoria, ā, he kaha teitei, he ātete hoki ki te waikura i te pāmahana rūma me te pāmahana tiketike.

Taupānga: E whakamahia ana mō te whakarewa i ngā koranu nikara-konu-moripenema, inā koa te whakarewa me te whakapuru i ngā koranu UNS N06625 me ētahi atu momo maitai me ngā maitai hiato koranu nikara-konu-moripenema, ā, ka taea hoki te whakamahi mō te whakarewa i te maitai Ni9% i raro i ngā āhuatanga pāmahana iti.

 

Te hanganga matū o te konganuku whakarewa (%):

C

Mn

Si

Cr

Ni

Mo

≤0.10

≤2.0

≤0.8

20.0 ~ 23.0

≥55.0

8.0 ~ 10.0

Fe

Cu

Nb + Ta

S

P

Ētahi atu

≤7.0

≤0.5

3.0 ~ 4.2

≤0.015

≤0.020

≤0.5

 

Ngā āhuatanga hangarau o te konganuku whakarewa:

tūemi whakamātautau

Te kaha o te kume

Mpa

Te kaha o te hua

Mpa

Te whakaroa

%

Kua whakamanahia

≥760

≥420

≥27

 

Iahiko e taunakitia ana:

Te whānui o te tokotoko

(mm)

2.5

3.2

4.0

Iahiko whakarewa

(A)

50 ~ 70

80 ~ 100

110 ~ 150

 

Pānui:

  1. Me tunu te hiko mō te 1 hāora i te pāmahana tata ki te 300℃ i mua i te mahi whakarewa. Whakamātauria te whakamahi i te pewa poto hei whakarewa;
  2. He mea nui kia horoia te waikura, te hinu, te wai me ngā poke i runga i ngā wāhanga whakarewa i mua i te whakarewa.

3. Whakamātauria te whakamahi i te pūngao aho iti i te wā e whakarewa ana, e whakarewa ana i ngā paparanga maha me ngā ara maha.

 

 