Waitohu Tyue Ngā Irahiko Whakarewa Āwhata Pai rawa atu AWS ENiCrFe-1 Nikara Whakarewa, Rākau Whakarewa

Whakaahuatanga Poto:

Ko te Ni307-1 (AWS ENiCrFe-1) he irahiko e ahu mai ana i te nikara, he iti te paninga hauwai konutai. Whakamahia te DCEP (irahiko au tika).


Taipitopito Hua

Ngā Tohu Hua

Irahiko Whakarewa Nikara me te Nikara

Ni307-1                                                     

GB/T ENi6062

AWS A5.11 ENiCrFe-1

Whakaahuatanga: He irahiko nikara te Ni307-1, he iti te paninga hauwai konutai. Whakamahia te DCEP (irahiko au tika). Nā te mea kei roto i te whakarewa he Nb, he pai te kirihou me te ātete ki te pakaru o te konganuku kua whakatakotoria.

Te Whakamahinga: Whakamahia mō te whakarewa i ngā koranu nikara-kōromium-rino (pēnei i te UNS N06600, UNS N06601) me te whakakikorua i te maitai. He pai ngā āhuatanga whakarewa rerekē. Ka taea hoki te whakamahi i te pāmahana mahi o te 980°C, engari ki te teitei ake te pāmahana i te 820°C, ka heke te ātete me te kaha o te waikura.

 

Te hanganga matū o te konganuku whakarewa (%):

C

Mn

Fe

Si

Cu

Ni

Cr

Nb + Ta

S

P

Ētahi atu

≤0.08

≤3.5

≤11.0

≤0.8

≤0.5

≥62.0

13.0 ~ 17.0

0.5 ~ 4.0

≤0.015

≤0.020

≤0.50

 

Ngā āhuatanga hangarau o te konganuku whakarewa:

tūemi whakamātautau

Te kaha o te kume

Mpa

Te kaha o te hua

Mpa

Te whakaroa

%

Kua whakamanahia

≥550

≥360

≥27

 

 

Iahiko e taunakitia ana:

Te whānui o te tokotoko

(mm)

2.5

3.2

4.0

5.0

Iahiko whakarewa

(A)

60 ~ 90

80 ~ 110

110 ~ 150

130 ~ 180

 

Pānui:

1. Me tunu te hiko mō te 1 hāora i te pāmahana tata ki te 300℃ i mua i te mahi whakarewa;

2. He mea nui kia horoia ngā waikura, te hinu, te wai, me ngā poke i runga i ngā wāhanga whakarewa i mua i te whakarewa. Whakamātauria te whakamahi i tētahi pewa poto hei whakarewa.

 

 