Rakau here AWS A5.1 E6013 (J421)

Whakaahuatanga Poto:

He pai mo te whakapiringa o te hanganga maitai waro iti AWS A5.1 E6013 (J421) fehokotaki'anga rakau, rawa mo te fehokotaki'anga o te maitai pereti kikokore ki te fehokotaki'anga discountinuous poto me te whakaritenga o te pai fehokotaki'anga haere.


Taipitopito Hua

Tohu Hua

He pai mo te whakapiringa o te hanganga maitai waro iti AWS A5.1 E6013 (J421) fehokotaki'anga rakau, rawa mo te fehokotaki'anga o te maitai pereti kikokore ki te fehokotaki'anga discountinuous poto me te whakaritenga o te pai fehokotaki'anga haere.

whakarōpūtanga:

ISO 2560-A-E35 0 RA 12

AWS A5.1: E6013

GB/T 5117 E4313

Āhuatanga:

Ko te AWS A5.1 E6013 (J421) he momo rutile electrode.Ka taea te whakakii i te puna hiko AC me te DC ka taea mo nga waahi katoa.He pai te mahi fehokotaki'anga rite pewa pūmau, iti mokamoka, ngāwari tango para me te reignition-kaha me ētahi atu. Rutile-cellulosic electrode ki pai te kaha fehokotaki'anga i roto i ngā tūranga katoa tae atu poutū ki raro.He pai te kaha ki te tarai-aputa me te arc-patu.Mo te wetewete me te utaina pai ake.Te kaupapa whanui mo te ahumahi me te hokohoko, te huihuinga me te toa toa.

aro:

Ko te tikanga, kaua e whakamaroke ano i te hiko i mua i te whakapiri.Ina pa ana ki te makuku, me whakamaroke ano ki te 150 ℃-170 ℃ mo te 0.5-1 haora.

Turanga Wea:

PA, PB, PC, PD, PE, PF

Ko te AWS A5.1 E6013 e pai ana mo nga hanganga raima i hangaia mai i te waro waro iti, he pai te mahi ki te whakapiri i nga pereti maitai angiangi me te iti, he pai hoki te mahi i roto i nga ahuatanga e hiahia ana ki te ahua pai me te ma.

Te Tito Matū o te Konuara Weld Katoa: (%)

Hangahanga matū

C

Mn

Si

S

P

Ni

Cr

Mo

V

Nga whakaritenga

≤0.10

0.32-0.55

≤0.30

≤0.030

≤0.035

≤0.30

≤0.20

≤0.30

≤0.08

Hua angamaheni

0.08

0.37

0.18

0.020

0.025

0.030

0.035

0.005

0.004

Nga Tikanga Miihini o te Metara Kua Pumau

Tūemi Whakamātautau

Rm (N/mm2)

Rel (N/mm2)

A (%)

KV2(J) 0 ℃

Nga whakaritenga

440-560

≥355

≥22

≥47

Hua angamaheni

500

430

27

80

Tohutoro Naianei (DC)

Diamita

φ2.0

φ2.5

φ3.2

φ4.0

φ5.0

Amperage

40 ~ 70

50 ~ 90

80 ~ 130

150 ~ 210

180 ~ 240

X-Ray Radiographic Inspection:

Taumata Ⅱ


  • Tōmua:
  • Panuku: