AWS A5.18 ER70S-6 Waro Wao Wire Fehokotakinga Waea Whakakii Kotara mo te Waea Hangaia Hau, Waea Maamaa

Whakaahuatanga Poto:

Ko te ER70S6 he waea whakarewa maitai e mau ana i nga taumata teitei ake o te konupora me te silicon atu i etahi atu tohu paerewa o te waea MIG hei whakaputa i nga paihere kounga teitei ina whakamahia ki runga i te rino paru, hinuhinu, waikura ranei.


Taipitopito Hua

Tohu Hua

Ko te ER70S6 he waea whakarewa maitai e mau ana i nga taumata teitei ake o te konupora me te silicon atu i etahi atu tohu paerewa o te waea MIG hei whakaputa i nga paihere kounga teitei ina whakamahia ki runga i te rino paru, hinuhinu, waikura ranei.Ko te ihirangi silicon teitei ka whakanui ake i te rere o te puna wai weld, na reira ka hanga he ahua maenee ake te pirepire me te hua i te iti o te huri i muri i te weld.I hangaia tenei waea ki te whakarato i te porosity-kore, he paihere x-ray i te kaha o te kaha (he paiherea) o nga waea waro maitai katoa.

Nga Tono Tikanga: nga tono toa whaanui he iti te pai, he waikura ranei, he pereti hinuhinu;te whakarewanga o te rino, te hanga whakaora ranei;kaupapa whare;rau whakarewa;taika;mahi hanga

AWS Class: ER70S6

Tiwhikete: AWS A5.18/A5.18M:2005

Kohanga: ER70S6

ASME SFA A5.18

Turanga Wea: F, V, OH, H

Inaianei: DCEP

Te Kaha Tana, kpsi:

70

Kaha Tuku, kpsi:

58

Whakaroa i te 2”%:

22

Matū Waea Angamaheni kia rite ki te AWS A5.18 (he nui te uara kotahi)

C

Mn

Si

P

S

Ni

Cr

Mo

V

Cu

0.06-0.15

1.40-1.85

0.80-1.15

0.025

0.035

0.15

0.15

0.15

0.03

0.50

Tawhā Welding angamaheni

Diamita

Tukanga

Volt

Tere Haerenga

Amps

Hau paruru

in

(mm)

(ipm)

.035

(0.9)

GMAW

23-26

11-22

160-300

Whakawhiti Rehu 98% Argon+2% Oxygen

.045

(1.2)

GMAW

23-29

12-21

170-375

Whakawhiti Rehu 98% Argon+2% Oxygen

1/16

(1.6)

GMAW

25-31

9-19

275-475

Whakawhiti Rehu 98% Argon+2% Oxygen

.023

GMAW

14-19

10-15

30-85

Whakawhiti Porohita Poto 98% Argon+2% Oxygen

.030

(0.8)

GMAW

15-20

12-24

40-130

Whakawhiti Porohita Poto 98% Argon+2% Oxygen

.035

(0.9)

GMAW

16-25

11-40

60-235

Whakawhiti Porohita Poto 98% Argon+2% Oxygen

.045

(1.14)

GMAW

18-23

12-22

90-290

Whakawhiti Porohita Poto 98% Argon+2% Oxygen

.035

(0.9)

GTAW

12-15

N/A

60-100

100% Argon

.045

(1.14)

GTAW

13-16

N/A

70-120

100% Argon

1/16

(1.6)

GTAW

12

N/A

100-160

100% Argon

1/16- 3/32

(1.6)-(2.4)

GTAW

12

N/A

120-250

100% Argon

1/8

(3.2)

GTAW

12

N/A

150-300

100% Argon


  • Tōmua:
  • Panuku: